ExxonMobil Exxon Aviation Oil EE Series 65

 

Subcategory: Fluid

Material Notes:
Aviation Oil EE is the brand name of a premium quality line of ashless-dispersant piston engine oils. Formulated with select, highly refined base oils together with ashless-dispersant and anti-oxidant additives, Aviation Oil EE is designed to satisfy the requirements of all major engine manufacturers under all climatic conditions. To meet a wide range of requirements, Aviation Oil EE is available as monogrades in four viscosity grades: 65, 80, 100, and 120.

Aviation Oil EE oils are designed to meet the requirements of modern aircraft piston engines used in commercial, military and private aircraft. Ashless-dispersant aviation engine oils have attained wide-spread use due to their ability to keep engines cleaner than non-dispersant oils. The four grades of Aviation Oil EE meet the requirements of major engine manufacturers where monograde ashless-dispersant engine oils are recommended. Aviation Oil EE products are U.S. Military approved under SAE J1899, which replaced MIL-L-22851D and are listed in the U.S. Military Qualified Products List QPL-1899. Specific viscosity grades are approved by Pratt and Whitney, Teledyne Continental Motors, and Textron Lycoming and included in their respective Qualified Products Lists. Appropriate viscosity grades are recommended for Curtis-Wright, Franklin, and Rolls-Royce engines. Compatibility: Aviation Oil EE Series is compatible with nondispersant mineral oils as well as with other ashless-dispersant oils that meet the requirements of MIL-L-22851D/SAE J1899. They can be used in high-time engines that have previously used a straight mineral oil. If this is done, however, it is advisable to carry out the oil-screen inspection recommended by the engine manufacturer.

Available Properties
  • Density
  • API Gravity
  • Viscosity Measurement
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Ash
  • Total Acid Number
  • Pour Point
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。