MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

ExxonMobil Mobilgrease EAL 101

 

Subcategory: Fluid; Lubricant

Key Words: NLGI Grade 1

Material Notes:
Mobilgrease EAL 101 and 102 are supreme performance greases designed specifically for applications which are environmentally sensitive. These leading products are biodegradable and virtually non-toxic greases formulated from a synthetic ester base fluid and a lithium soap thickener. The wax-free nature of the synthetic base fluid, together with its low traction coefficient, provide excellent low temperature pumpability and very low starting and running torque - a significant benefit considering many environmentally sensitive applications are located outdoors. Mobilgrease EAL 101and 102 were formulated for multipurpose outdoor applications where grease leakage or run out could contaminate soil, groundwater or surface water systems. They can be used for indoor applications where grease leakage could enter plant water systems. They are recommended for plain and rolling element bearings and couplings that operate at temperatures from -30ºC to 120ºC. Mobilgrease EAL 101and 102 are NLGI grade 1 and 2 respectively; both have ISO VG 100 base oils. Extensive field evaluation and commercial experience with these products around the world has confirmed good performance in a variety of applications ranging from marble quarry chain saws to hydro-turbines. Even though they are designed for environmental benefits, Mobilgrease EAL 101 and 102 stand up to very demanding performance standards and help extend equipment life and keep equipment running reliably and efficiently.

Mobilgrease EAL 101and 102 are two members of a family of Mobil Environmental Awareness Lubricants (EAL) specifically designed for applications where contamination of the environment is a risk. Mobilgrease EAL 101 (NLGI Grade 1) and 102 (NLGI Grade 2) are multipurpose greases formulated with an ISO VG 100 base fluid. They are designed for the lubrication of equipment in environmentally sensitive areas, including: Marine equipment; Water treatment plants; Dams, locks and water ways; Construction equipment; Farm machinery

Available Properties
  • Kinematic Viscosity at 40°C (104°F)
  • Four Ball Extreme Pressure, Weld Load
  • Four Ball Wear
  • Penetration
  • Timken Test
  • Dropping Point
  • Biodegradability Shake-Flake Test
  • Color
  • Copper Strip Corrosion, ASTM D130
  • Corrosion Prevention, ASTM D1743
  • Emcor/SKF Water Wash Test, IP 220
  • Soap/Thickener Type
  • Water Washout, ASTM D1264, wt%
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。