ExxonMobil Mobilgrease 27

 

Subcategory: Fluid; Lubricant

Key Words: NLGI Grade 1.5

Material Notes:
Mobilgrease 27 is a high performance, aviation grease designed to combine the unique features of a synthetic ester base fluid with a lithium soap thickener. Its consistency is between an NLGI No. 1 and No. 2 grease. It offers outstanding performance over a wide temperature range. The thickener system provides excellent structural stability and resistance to water wash. The properties of the base oil, combined with selected additives, provide outstanding protection against rust, corrosion, wear and high temperature degradation. The synthetic base oil allows for low-temperature mobility/pumpability and very low starting and running torque values.

Mobilgrease 27 is a true multipurpose aviation grease intended for use in highly loaded gears and actuators as well as instruments, high speed bearings (though not recommended for wheel bearings), and general airframe lubrication over temperatures from –100ºF to 250ºF. Mobilgrease 27 is also an excellent choice for applications where a smooth, low noise, wide temperature range lubricating grease is required, such as in miniature precision bearings. Mobilgrease 27 contains a synthetic ester and should not be used in contact with incompatible seal materials. It may soften natural rubber, neoprene, certain electrical insulation materials and paints. Mobilgrease 27 meets the requirements and is approved against U.S. Military Specification MIL-PRF-23827, Grease, Aircraft and Instrument, Gear and Actuator Screw, Type I (Grease thickened with metallic soap). It is listed in the QPL-23827 Qualified Products List. In addition, Mobilgrease 27 may be used in all applications where MIL-G-3278, MIL-G-7118, MIL-G-7421, MIL-G-15793 and MIL-G-23827 are specified, subject to approval by the aircraft manufacturer. It is a NATO Code Number G-354 grease.

Available Properties
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Oxidative Stability
  • Evaporation Loss
  • Storage Temperature
  • Four Ball Extreme Pressure, Load Wear Index
  • Penetration
  • Oil Separation
  • Dropping Point
  • Color
  • Copper Strip Corrosion, ASTM D4048
  • Corrosion Prevention, ASTM D1743
  • Gear Wear, FTM 335
  • Grease Life, DIN 51821 (FE-9), hours
  • Low Temperature Torque, ASTM D1478, g-cm
  • Particle Count, 25-50 microns
  • Soap/Thickener Type
  • Structure
  • Water Washout, ASTM D1264, wt%
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。