Gwent Electronic Materials (GEM) Conductor for Polymer Substrate Materials: C2020606D1 Silver Carbon Ink

 

Subcategory: Additive/Filler for Polymer; Adhesives, Sealants, and Coatings

Material Notes:
C2020606D1 is a screen printable, conductive Silver Carbon Ink, designed for applications on Polyester and ITO-coated Polyester Films. This is an easy processing paste, consisting of finely divided silver and carbon particles dispersed in a thermoplastic resin system. This ink is compatible with C2020522D1 Silver Ink, which can be used in areas where sheet resistivity is critical.

The ink has been made at a ready to use viscosity and should be thoroughly stirred before use avoiding introduction of air bubbles. It can be printed on automatic and semi automatic screen printers.

Information provided by Gwent Electronic Materials Ltd.

Available Properties
  • Density
  • Viscosity
  • Storage Temperature
  • Volume Resistivity
  • Surface Resistivity per Square
  • Drying Temperature
  • Dry Time
  • Shelf Life
  • Abrasion Resistance - Pencil Hardness
  • Coverage cm2/g
  • Printing Mesh counts/inch
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。