MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Gwent Electronic Materials (GEM) Counter Electrode Material: C2040922D1 Silver Counter Electrode Paste

 

Subcategory: Ceramic/Metallic Coating; Adhesives, Sealants, and Coatings

Material Notes:
C2040922D1 is a screen printable silver paste designed as a counter electrode in electrochemical Biosensors. This is used as a counter electrode in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries, in conjunction with working electrode - (C2040706D7 Carbon Paste). This product can be used to increase the conductivity of the carbon/graphite by printing tracks underneath.

The paste is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The paste should be gently stirred before use avoiding introduction of air bubbles. It is a Polymer System for printing on polyester, PVC, Polycarbonate etc and on alumina.

Information provided by Gwent Electronic Materials Ltd.

Available Properties
  • Solids Content
  • Viscosity
  • Thickness
  • Storage Temperature
  • Surface Resistivity per Square
  • Dry Time
  • Shelf Life
  • Coverage cm2/g
  • Fineness of Grind, microns
  • Printing Mesh counts/inch
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。