Texaco Aquagear® EP 220

 

Subcategory: Fluid

Close Analogs: CPS Number: 222657; MSDS Number: 8641

Material Notes:
Texaco Aquagear EP oils deliver value through:

  • Long equipment life — Effective sulfur-phosphorus extreme-pressure additives provide high film thickness that protects gear teeth from wear and premature failure.
  • Long oil life — Special additives and base oil formulations prevent product degradation when operating in severe conditions that lead to rapid oxidation and thermal stress — providing long service life of the oil.
  • Flexibility to use in wet conditions — Quickly forms stable emulsions with water to prevent separated water from corroding equipment, and reduces water corrosion on either steel (rust) or nonferrous metals (including copper and its alloys) in gear sets.
  • Cold weather reliability — Pour point is depressed to provide good cold flow performance at low temperature conditions.

Texaco Aquagear EP oils are multipurpose gear lubricants.

They are formulated with highly refined, high viscosity index paraffinic base oils and a new generation sulfurphosphorus additive system. Texaco Aquagear EP oils contain extreme pressure, antiwear and emulsibility additives; oxidation, rust, corrosion and foam inhibitors; a pour point depressant; and a metal deactivator to protect copper or copper alloys from corrosion.

They are specifically designed to meet or exceed the performance requirements of Joy Technologies specifications for transmission oils.

Texaco Aquagear EP oils high film strength and load-carrying capacity. Gear teeth are protected from wear, all types of surface distress, and premature failure.

They provide improved thermal and oxidation stability to prevent degradation under severe operating conditions and provide longer lubricant life.

They are designed to form a stable emulsion with contaminating water.

Texaco Aquagear EP oils are recommended for use in Joy Technologies transmissions or other similar applications where water emulsifying gear oils are required.

Texaco Aquagear EP oils meet Joy specifications TO-MEP (ISO 220), TO-HEP (ISO 320) and TO-HD (ISO 460).

Texaco Aquagear EP oils can be used in industrial applications where overloading, severe operating conditions, high lubricant operating temperatures, or other problems are encountered.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Available Properties
  • API Gravity
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Falex Load Test
  • Pour Point
  • Flash Point
  • Oxygen Index
  • Corrosion, Copper Strip
  • Emulsibility, mL H2O
  • Foaming Stability, mL
  • Foaming Tendency, mL
  • FZG Pass Stage
  • Rust Prevention
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。