Texaco Multigear® EP SAE 80W-90

 

Subcategory: Fluid

Close Analogs: CPS Number: 222316; MSDS Number: 8628

Material Notes:
Texaco Multigear EP oils deliver value through:

  • Improved durability — Specially formulated to stand up to the demands of severe service applications.
  • Extended gear life — Extreme pressure properties protect hypoid and other types of gears from scuffing and wear under heavily loaded conditions.
  • Long lubricant life — Outstanding thermal and oxidation stability allow high temperature operation with long lubricant life without the formation of sludge and deposits.
  • All-weather protection — Multiviscosity characteristics assure proper gear lubrication at both low and high ambient temperatures.
  • Corrosion and rust protection — Effective inhibitor package prevents rusting or corrosion of gears and bearings surfaces.

Texaco Multigear EP oils are multipurpose lubricants.

They are made with:

  • Highly refined base stocks
  • A carefully balanced additive package to provide maximum gear protection, long lubricant life and excellent field performance
  • Sulfur-phosphorus extreme pressure additives that provide superior thermal and oxidation stability
  • Rust and corrosion inhibitors, a foam inhibitor, and a pour point depressant

The highly refined base stocks and various inhibitors in the additive package assure a well-balanced lubricant and long gear and bearing life with maximum durability.

Texaco Multigear EP oils are recommended for use in all spiral bevel and hypoid differentials, power dividers, and oil-lubricated steering axle wheel bearings.

They are designed for complete refill and make-up of all passenger car, light duty and heavy duty truck transmissions, conventional differentials and steering gears.

Their multiviscosity characteristics allow their use in equipment operating over a broad ambient temperature range. This means good cold flow properties and gear protection.

Texaco Multigear EP oils meet the performance requirements of:

  • API Service Categories MT-1, GL-4, and GL-5
  • Are qualified for SAE J 2360 (formerly known as MIL-PRF-2105E)

They also meet the requirements of:
  • A Mack GO-J fluid
  • Rockwell 0-76D (SAE 80W-90), 0-76-A (SAE 85W-140)

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Available Properties
  • API Gravity
  • Brookfield Viscosity
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Pour Point
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。