MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Texaco URSA® Premium TDX SAE 15W-40

 

Subcategory: Fluid

Close Analogs: CPS Number: 222153; MSDS Number: 8603

Material Notes:
Texaco Ursa Premium TDX SAE 15W-40 delivers value through:

  • Reduced wear — Prolonging component life and providing reduced maintenance costs.
  • Improved engine cleanliness — Providing efficient operation and reduced fuel consumption.
  • Extended drain capability — Reducing operating costs (approved by Mack, Cummins, Mercedes Benz, MTU, MAN).
  • Oil consumption control — Controls wear and piston deposits resulting in reduced emissions.
  • Engine durability even under arduous extended oil drain periods.
  • Long engine life resulting from additives that protect highly loaded parts from scuffing and wear.
  • Extensive field testing and service use — A proven track record of meeting customer and OEM requirements.
  • Extended filter life — Whether in modern electronically controlled engines or older models, helps extend filter life by handling the soot that clogs filters and increases valve train wear.

Texaco Ursa Premium TDX SAE 15W-40 is a super high performance diesel engine oil (SHPD) specially designed for use in heavy duty turbo-charged diesel engines with extended drain interval approval for various engine manufacturers.

Texaco Ursa Premium TDX SAE 15W-40 is recommended for four-stroke naturally aspirated, turbocharged, and supercharged diesel engines in all types of service.

It is ideal for mixed commercial fleets, farm machinery, construction equipment, marine and other off-highway applications as it can also be used in four-stroke gasoline engines.

Texaco Ursa Premium TDX SAE 15W-40 can be used in powershift transmissions requiring Caterpillar TO-2 or Allison C4 fluids.

Texaco Ursa Premium TDX 15W-40 meets:

  • API Service Categories
    • CI-4, CH-4, CG-4, CF-4, CF, CD1
    • SL, SJ, SH, SG1
  • ACEA European Oil Sequences
    • E7, E5, E3, E2
  • Major diesel engine manufacturers requirements
    • Cummins CES 20078, 20077, 20076, 20072
    • DDC/MTU Series 2000/4000 Type 2
    • EMA LRG-1
    • Global DHD-1
    • JASO DH-1
    • Mack EO-N Premium Plus, EO-M Plus, EO-M, EO-L PLUS, EO-L
    • MAN M3275
    • Mercedes Benz 228.3
    • MTU Category 2
    • Volvo VDS-3, VDS-2
  • Performance requirements of
    • Allison C4 Fluids
    • Caterpillar TO-2
  • Manufacturers performance requirements:
    • Chrysler MS 6395-G
    • Ford ESE-M2C153-E
    • General Motors GM 6094-M
  • Department of Defense Commericial Item Description (CID)
    • A-A-52039A2

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Obsolete Specification.
  2. Replaces MIL-L-46152E.
  3. Available Properties
    • API Gravity
    • Viscosity
    • Viscosity Measurement
    • Kinematic Viscosity at 40°C (104°F)
    • Kinematic Viscosity at 100°C (212°F)
    • Ash
    • Total Base Number
    • Pour Point
    • Flash Point
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。