Texaco Almag® Oil

 

Subcategory: Fluid

Close Analogs: CPS Number: 221564; MSDS Number: 10275

Material Notes:
Texaco Almag oil delivers value through:

  • Low viscosity that provides faster wetting of metal surfaces and penetration to the cutting zone.
  • Excellent cooling properties, carrying heat away from the cutting zone.
  • Excellent lubricity at the chip-tool interface, reducing frictional heat, improving tool life and surface finish.

Texaco Almag oil is a low viscosity, nonactive cutting oil for use in light duty machining and grinding operations on ferrous and nonferrous metals. It is particularly useful on aluminum, magnesium and their alloys.

Texaco Almag Oil is a straight mineral oil. It is a light-colored oil that possesses excellent cooling properties and high dielectric strength. Because of its composition, it is nonstaining for ferrous and nonferrous surfaces. It gives good wetting and penetration of cutting surfaces.

Texaco Almag oil is recommended for light duty machining and grinding operations on ferrous and nonferrous metals. It is excellent for aluminum, magnesium and their alloys. It is particularly suited for the machining of magnesium where the use of a water-based fluid could create a fire hazard.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Available Properties
  • API Gravity
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Pour Point
  • Flash Point
  • Fatty Oil
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。