Texaco Quenchtex® MM

 

Subcategory: Fluid

Close Analogs: CPS Number: 221508; MSDS Number: 10310

Material Notes:
Texaco Quenchtex oils deliver value through:

  • Controlled cooling of metals — Combines the high initial quenching speed of water with slow final quenching speed of oil.
  • Safety — High flash point and fire point minimize the possibility of fire problems.
  • Stable additive package — Minimal loss of additives due to extended use.
  • Minimal oil carryout — The light viscosity of this oil allows quick drainage from metal parts preventing carryout.
  • Excellent thermal stability — Provides high heat resistance to oxidation and thickening.
  • Deeper, more uniform hardening due to controlled cooling of metals.

Texaco Quenchtex oils are highly refined, paraffinic based quenching oils.

They provide controlled cooling of steel which is important in steel hardening. When quenching is started, Texaco Quenchtex oils provides a high initial cooling rate inducing maximum hardness, yet once the critical transformation temperature is passed, the ideal fluid cooling rate decreases to eliminate the possibility of stresses and metal distortion.

Texaco Quenchtex MM is used in quenching and mar-quenching operations and is recommended for the production of very hard parts, especially where distortion of the quenched parts cannot be tolerated.

These oils resist the oxidizing effects of quenching and are less sensitive to the effects of agitation. They are highly heat resistant. No additive replacement is required and, in normal service, they retain the original viscosity indefinitely.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Available Properties
  • API Gravity
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Pour Point
  • Flash Point
  • Quench Time, s
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。