Havoline® Extended Life Anti-Freeze/Coolant

 

Close Analogs: CPS Number: 227994; MSDS Number: 10299

Material Notes:
In service Havoline Extended Life Anti-Freeze/Coolant provides:

  • Meets GM 6277M--GM’s Long Life Coolant specification
  • 5 year or 150,000 mile service interval
  • Provides effective, long term corrosion protection for aluminum, brass, cast iron, steel, solder and copper
  • Protects against winter freeze up and minimizes the chance of summer boil over
  • Compatible with water pump seal materials and minimizes the formation of abrasive dissolved solids
  • Storage stable for at least eight years
  • No silicate dropout or gel formation during use or storage
  • 100% biodegradable in its pure unused form
  • Excellent heat transfer properties
  • Nitrite-, borate-, phosphate-, nitrate- and amine-free
  • Outstanding hot surface aluminum protection
  • Superior protection in high operating temperatures
  • Compatible with conventional antifreeze. Dilution with conventional antifreeze will reduce extended life benefits. ChevronTexaco recommends that this product not be diluted by more than 10% with conventional coolants.

Havoline Extended Life Anti-Freeze/Coolant is a singlephase, ethylene glycol type universal automotive engine coolant based on a Texaco’s patented long life organic corrosion inhibitor system.

Havoline Extended Life Anti-Freeze/Coolant is manufactured from ethylene glycol and a highly effective long term corrosion inhibitor package based on carboxylate technology. This inhibitor system eliminates the need for silicates, phosphates, borates, nitrites, nitrates and amine additives traditionally used for this purpose.

The replacement of these inhibitors is significant for water pump life because many of these conventional inhibitors have been shown to be abrasive to water pump seals. In comparison field tests with conventional coolants in taxi fleets, Havoline Extended Life Anti-Freeze/Coolant significantly reduced the need to replace water pumps during the 100,000 mile test.

In addition to fleet tests, this product has also been tested by a major manufacturer of water pump seals, and has been found to be more compatible with the seals than any other coolant tested.

Havoline Extended Life Anti-Freeze/Coolant is a universal engine coolant that incorporates patented organic acid corrosion inhibitor technology. This coolant meets both ASTM D 3306 for automotive service and ASTM D 4985 for heavy-duty diesel service. It is a nitrite-, nitrate-, phosphate-, silicate-, borate and amine-free formulation which uses Texaco’s patented carboxylate technology to provide maximum protection of the six basic metal alloys found in most heat transfer systems. Since the coolant contains no phosphates or silicates, hard water deposits in the cooling system are almost eliminated. The low level of abrasive dissolved solids in Havoline Extended Life Anti-Freeze/Coolant results in improved water pump seal life.

The life of a coolant in an automobile engine is limited by the corrosion protection ability of the corrosion inhibitors. The main corrosion inhibitors in Havoline Extended Life Anti-Freeze/Coolant have been shown to remain above 95% of their original concentration after 150,000 miles in automobiles. This allows much longer intervals between coolant changes without worrying about loss of corrosion protection.

Used Havoline Extended Life Anti-Freeze/Coolant was tested in laboratory controlled corrosion tests for new coolants after it had already been in service for more than 100,000 miles. The used Havoline Extended Life Anti-Freeze/Coolant passed the ASTM D 1384 requirements for glassware corrosion with results equivalent to new coolants and also passed the ASTM D 4340 Aluminum Hot Surface Test for new coolant. Havoline Extended Life Anti-Freeze/Coolant represents the next generation of universal engine coolants. This coolant is suitable for a five year or 150,000 miles service life in automotive applications.

Note: These products are not to be used to protect the inside of potable water systems against freezing.

Havoline Extended Life Anti-Freeze/Coolant is recommended for use in the cooling systems of all types of automotive engines. This product meets ASTM D 3306 for automotive service and ASTM D 4985 for heavy-duty diesel service.

Havoline Extended Life Prediluted 50/50 Anti-Freeze/Coolant meets ASTM D 4656 for automotive preblend and ASTM D 5345 for heavy-duty preblend.

Note: For optimum year round protection against freezing, boiling, and corrosion, a 50 percent Havoline Extended Life Anti-Freeze/Coolant solution (1 part antifreeze/1 part water) is recommended. For maximum protection against freezing in extremely cold areas, a 60 percent solution (3 parts anti-freeze/2 parts water) can be used. Concentrations greater than 67 percent or less than 40 percent are not recommended.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Negative indicates net gain.

Available Properties
  • Specific Gravity
  • pH
  • Melting Point
  • Appearance
  • Glassware Corrosion Test, Aluminum
  • Glassware Corrosion Test, Brass
  • Glassware Corrosion Test, Copper
  • Glassware Corrosion Test, Iron
  • Glassware Corrosion Test, Solder
  • Glassware Corrosion Test, Steel
  • Reseve Alkalinity (mL)
  • Silicate %
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。