Texaco Texcool® P-200 Series P 205

 

Close Analogs: CPS Number: 227972; MSDS Number: 10715

Material Notes:
In service Texaco Texcool P 200 provides:

  • Silicate free
  • Excellent heat transfer properties
  • Superior corrosion protection for brass, copper, solder, steel and cast iron
  • Nitrite-free, amine-free
  • Mixes readily with clean tap water
  • 100% biodegradable in its pure unused form

Texaco Texcool P 205 is a 50 volume % mixture of Texaco Texcool P 200 and 50 volume % deionized water.

Texaco Texcool P 200 is a single phase, propylene glycol (USP) based product blended with a premium quality additive package. It is a silicate free coolant designed and approved for use in immersion or spray freezing equipment of packaged poultry or meat under the Federal Meat and Poultry Products Inspection Program. Texaco Texcool P 200 should not be used for automotive or nonstationary heavy duty diesel applications. This product provides antifoam properties, and rust and corrosion protection for brass, copper, solder, steel and cast iron. It mixes readily with any clean tap water and is compatible with cooling system filters and supplemental additives.

Texaco Texcool P 200 is free of nitrites and amines.

Texaco Texcool P 200 is an inhibited propylene glycol (USP) based product that is used as an industrial coolant and heat transfer agent. In non-USDA applications, Texaco Texcool P 200 may be used in applications where incidental contact with food is possible. This product is not intended for use as a food component or additive. The inhibitor system is designed to protect brass, copper, solder, steel, cast iron, aluminum, and other metals commonly found in industrial cooling and heating systems. A foam inhibitor is included to minimize foaming tendencies during service.

Extensive laboratory simulated service and actual service tests have proven the effectiveness of Texaco Texcool P 200 coolant in preventing corrosion. Use of Texaco Texcool P 200 coolant for heat transfer applications in place of brine solutions or uninhibited glycolwater solutions lowers maintenance costs and improved heat transfer.

Texaco Texcool P 200 meets the requirements of the U.S. Department of Agriculture (USDA) for use in the immersion or spray freezing equipment of packaged poultry or wrapped meat under the Federal Meat and Poultry Products Inspection Program.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Available Properties

We're sorry, but our sources do not report
any other information for this material.

  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。