Latrobe BG42® Stainless Knife Steel (AMS 5749)
Subcategory: Ferrous Metal; High Carbon Steel; Metal; Stainless Steel; Tool Steel; Martensitic
Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
| Component | Wt. % |  | | | C | 1.15 | | | Cr | 14.5 | | | Fe | 78.35 | | | Mn | 0.5 | | | Mo | 4 | | | Si | 0.3 | | | V | 1.2 | |
|
Material Notes: LESCALLOY® BG42® VIM VAR is a double vacuum melted martensitic stainless high speed steel designed for critical aerospace structural components and highperformance bearings. The steel is vacuum induction melted (VIM) and vacuum arc remelted (VAR) to provide the extremely high cleanliness level required for these fatigue-critical applications. When manufactured in sheet form, BG42 has proven to be an excellent knife steel. The very good wear resistance and corrosion resistance result in knife blades which exhibit excellent edge retention and long life. The molybdenum in the steel enhances the corrosion resistance provided by the high chromium content. In addition, the hromium, molybdenum, and vanadium contents provide approximately 19% carbide volume in the steel. This high carbide volume and the presence of very hard vanadium carbides enhance the wear resistance and edge retention of knife blades. The excellent edge retention and good corrosion resistance establish BG42 as an upgrade material compared to the
| Mechanical Properties | Metric | English | Comments |
|
| Hardness, Rockwell C | 59 | 59 | Oil Quenched from 1149°C, 10 minutes |
| Hardness, Rockwell C | 59.5 | 59.5 | Oil Quenched from 1066°C, 15 minutes |
| Hardness, Rockwell C | 62.5 | 62.5 | Oil Quenched from 1093°C, 15 minutes |
| Machinability | 55 - 60 % | 55 - 60 % | 1% Carbon Steel |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.

|