MatWeb Conversions for Engineering Units
Welcome to MatWeb's automatic unit converter. Simply enter the value that you would like to convert ("1" is the default), choose
the units of measure from which you would like to convert from the drop-down list, then press the "Convert" button. MatWeb's conversion
engine will return a list of other units with the appropriate converted values.
MatWeb has also provided a conversion table for converting between English and Metric units.
To Convert From: |
To: |
Multiply By: |
| lbf/in2 (psi) |
pascal (Pa) |
6894.757 |
| pascal (Pa) |
lbf/in2 (psi) |
1.4504E-4 |
| g/cm3 |
lb/ft3 |
62.427974 |
| lb/ft3 |
kg/m3 |
16.01846 |
| lb/in3 |
kg/m3 |
27,679.90 |
| lb/ft3 |
g/cm3 |
0.01601846 |
| volts/mil |
kV/mm |
0.039370 |
| mil (0.001 inch) |
cm |
2.54E-3 |
| cm |
mil |
393.70 |
| MPa(m1/2) |
psi(in1/2) |
910.06 |
| J/(g-°C) |
BTU/(lb-°F) |
0.239006 |
| BTU/(lb-°F) |
J/(g-°C) |
4.184000 |
| joule (J) |
cal (thermochemical) |
0.2390057 |
| cal (thermochemical) |
joule (J) |
4.184000 |
| joule (J) |
BTU (thermochemical) |
9.4845E-4 |
| BTU (thermochemical) |
joule |
1054.350 |
| µm/(m-°C) |
µin/(in-°F) |
0.55556 |
| µin/(in-°F) |
µm/(m-°C) |
1.80 |
| cm3/Kg |
in3/lb |
0.027680 |
| in3/lb |
cm3/kg |
36.127 |
| W/(m K) |
BTU in /(hr ft2 F) |
6.9334713 |
| BTU in /(hr ft2 F) |
W/(m K) |
0.1441314 |
| (J m)/(min m2 C) |
W/(m-K) |
0.016667 |
| W/(m-K) |
(J m)/(min m2 C) |
60 |