Solvay Advanced Polymers Radel® A AG-320 Polyethersulfone
Subcategory: Polyethersulfone; Polymer; Thermoplastic
Close Analogs: This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.
Key Words: PES
Material Notes:
Data provided by the manufacturer, Amoco Corporation. For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Metric | English | Comments |
|
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
Water Absorption | 0.45 % | 0.45 % | in 24 hours per ASTM D570 |
Mechanical Properties |
|
Tensile Strength, Yield | 105 MPa | 15200 psi | ASTM D638 |
Elongation at Break | 3.2 % | 3.2 % | ASTM D638 |
Elongation at Yield | 3.2 % | 3.2 % | ASTM D638 |
Tensile Modulus | 5.69 GPa | 825 ksi | ASTM D638 |
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
Flexural Yield Strength | 162 MPa | 23500 psi | ASTM D790 |
Izod Impact, Notched | 0.6 J/cm | 1.12 ft-lb/in | ASTM D256 |
Tensile Impact Strength | 70 kJ/m² | 33.3 ft-lb/in² | |
Electrical Properties |
|
Electrical Resistivity | 1e+016 ohm-cm | 1e+016 ohm-cm | ASTM D257 |
Dielectric Constant | 3.8 | 3.8 | at 1 kHz; ASTM D150 |
Dielectric Constant, Low Frequency | 3.8 | 3.8 | at 1 kHz; ASTM D150 |
Dielectric Strength | 18 kV/mm | 457 kV/in | Thickness 0.32 mm (13 mils); ASTM D149 |
Dissipation Factor | 0.002 | 0.002 | at 1 kHz; ASTM D150 |
Dissipation Factor, Low Frequency | 0.002 | 0.002 | at 1 kHz; ASTM D150 |
Thermal Properties |
|
CTE, linear 20°C | 31 µm/m-°C | 17.2 µin/in-°F | in flow direction. ASTM E381 |
CTE, linear 20°C Transverse to Flow | 31 µm/m-°C | 17.2 µin/in-°F | ASTM E381 |
Deflection Temperature at 1.8 MPa (264 psi) | 214 °C | 417 °F | ASTM D648 |
UL RTI, Electrical | 190 °C | 374 °F | 1.57 mm |
UL RTI, Mechanical with Impact | 190 °C | 374 °F | 1.57 mm |
UL RTI, Mechanical without Impact | 190 °C | 374 °F | 1.57 mm |
Flammability, UL94 | V-0 | V-0 | 0.8 mm |
Flammability, UL94 | V-0 | V-0 | 0.8 mm |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|