MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

COMSOL CD

Solvay Advanced Polymers Radel® A AG-230 Polyethersulfone

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polyethersulfone; Polymer; Thermoplastic

Close Analogs: This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.

Key Words: PES

Material Notes:

Data provided by the manufacturer, Amoco Corporation.

For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.

Physical PropertiesMetricEnglishComments
Density1.58 g/cc0.0571 lb/in³ ASTM D792
Water Absorption0.42 %0.42 % in 24 hours per ASTM D570

Mechanical Properties
Tensile Strength, Yield126 MPa18300 psi ASTM D638
Elongation at Break1.9 %1.9 % ASTM D638
Elongation at Yield1.9 %1.9 % ASTM D638
Tensile Modulus8.62 GPa1250 ksi ASTM D638
Flexural Modulus8.07 GPa1170 ksi ASTM D790
Flexural Yield Strength179 MPa26000 psi ASTM D790
Izod Impact, Notched0.7 J/cm1.31 ft-lb/in ASTM D256
Tensile Impact Strength70 kJ/m²33.3 ft-lb/in² 

Electrical Properties
Electrical Resistivity1e+016 ohm-cm1e+016 ohm-cm ASTM D257
Dielectric Constant4.14.1 at 1 kHz; ASTM D150
Dielectric Constant, Low Frequency4.14.1 at 1 kHz; ASTM D150
Dielectric Strength18 kV/mm457 kV/in Thickness 0.32 mm (13 mils); ASTM D149
Dissipation Factor0.0020.002 at 1 kHz; ASTM D150
Dissipation Factor, Low Frequency0.0020.002 at 1 kHz; ASTM D150

Thermal Properties
CTE, linear 20°C31 µm/m-°C17.2 µin/in-°F in flow direction. ASTM E381
CTE, linear 20°C Transverse to Flow31 µm/m-°C17.2 µin/in-°F ASTM E381
Deflection Temperature at 1.8 MPa (264 psi)213 °C415 °F ASTM D648
UL RTI, Electrical190 °C374 °F 1.57 mm
UL RTI, Mechanical with Impact190 °C374 °F 1.57 mm
UL RTI, Mechanical without Impact190 °C374 °F 1.57 mm
Flammability, UL94V-0V-0 0.8 mm
Flammability, UL94V-0V-0 0.8 mm
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。