Advanced Elastomer Systems Santoprene® 121-50 M100 Thermoplastic Rubber
Subcategory: Elastomer, TPE; Polymer; Thermoplastic
Material Notes: A black thermoplastic high-flow elastomer for excellent injection molding performance with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and high quality SEBS compounds. It is polyolefin-based and UV stable. Key Features: Fast, easy injection molding, especially for complex part geometries; Good sealing performance; Excellent surface aspect; Excellent elastic recovery up to 100°C (212°F); Minimal part warpage; Can be injected at lower molding temperatures or at lower injection pressures Additional processing comments: This thermoplastic rubber is a shear-dependent material that can be processed on conventional thermoplastic equipment for injection molding. Material can be recycled. SANTOPRENE rubber is incompatible with acetal and PVC. Values below are for injection molded plaques, side gated, 82.6 mm x 117.5 mm x 3.0 mm. Tensile properties measured across flow. Data provided by Advanced Elastomer Systems.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Metric | English | Comments |
|
Density | 0.91 g/cc | 0.0329 lb/in³ | TPE-0105 (ASTM D792) |
Mechanical Properties |
|
Hardness, Shore A | 50 | 50 | 5 Second; TPE-0169 (ASTM D 2240) |
Tensile Strength, Ultimate | 3.5 MPa | 508 psi | TPE-0153 (ASTM D 412) |
Elongation at Break | 340 % | 340 % | TPE-0153 (ASTM D 412) |
100% Modulus | 0.0018 GPa | 0.261 ksi | TPE-0153 (ASTM D 412) |
Compression Set | 22 % | 22 % | 23°C, 168 hrs.; TPE-0016 (ASTM D 412) |
Compression Set, Elevated Temperature | 32 % | 32 % | 70°C for 168 hrs.; TPE-0016 (ASTM D 412) |
Compression Set, Elevated Temperature | 40 % | 40 % | 100°C, 168 hrs.; TPE-0016 (ASTM D 412) |
Tensile Set | 10 % | 10 % | 23°C, 168 hrs.; TPE-0053 (ASTM D 412) |
Thermal Properties |
|
Brittleness Temperature | Max -60 °C | Max -76 °F | TPE-0089 (ASTM D 746) |
Processing Properties |
|
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Drying Temperature | 82 °C | 180 °F | Desiccant drying for 3 hours recommended |
Dry Time | 3 hour | 3 hour | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|