Advanced Elastomer Systems Santoprene® 251-70 W232 Thermoplastic Rubber
Subcategory: Elastomer, TPE; Polymer; Thermoplastic
Material Notes: A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It does not contain polybrominated diphenylethers (PBDEs) and can be processed using injection molding, extrusion, blow molding or other melt processing techniques. Key Features: Excellent flex fatigue resistance; Excellent ozone resistance; Limiting oxygen index, 26% Additional processing comments: This thermoplastic rubber is a shear-dependent material that can be processed on conventional thermoplastic equipment for injection molding, extrusion, or blow molding. For extrusion, a general purpose screw with a compression ratio of 2.5 to 3.0 is recommended. Material can be recycled. SANTOPRENE rubber is incompatible with acetal and PVC. Values below are for injection molded plaques, side gated, 82.6 mm x 117.5 mm x 3.0 mm. Tensile properties measured across flow. Data provided by Advanced Elastomer Systems.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Metric | English | Comments |
|
Density | 1.23 g/cc | 0.0444 lb/in³ | TPE-0105 (ASTM D792) |
Mechanical Properties |
|
Hardness, Shore A | 70 | 70 | 5 Second; TPE-0169 (ASTM D 2240) |
Tensile Strength, Ultimate | 5.5 MPa | 798 psi | TPE-0153 (ASTM D 412) |
Elongation at Break | 460 % | 460 % | TPE-0153 (ASTM D 412) |
100% Modulus | 0.0026 GPa | 0.377 ksi | TPE-0153 (ASTM D 412) |
Thermal Properties |
|
Brittleness Temperature | Max -57 °C | Max -70.6 °F | TPE-0089 (ASTM D 746) |
Oxygen Index | 26 % | 26 % | TPE-0112 (ASTM D 2863) |
Processing Properties |
|
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Drying Temperature | 82 °C | 180 °F | Desiccant drying for 3 hours recommended |
Dry Time | 3 hour | 3 hour | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|