MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

BASF Ecoflex F BX 7011 Biodegradable, Aliphatic Aromatic Copolyester

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Film; Polyester, TP; Polymer; Thermoplastic

Material Notes:
Information provided by BASF Corporation.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesMetricEnglishComments
Density1.26 g/cc0.0455 lb/in³ ISO 1183
Moisture Vapor Transmission140 cc-mm/m²-24hr-atm356 cc-mil/100 in²-24hr-atm cc/m2/day (Thickness Unknown); DIN 53122
Oxygen Transmission Rate1600 cc/m²/day103 cc/100 in²/day 23°C/0% RH; DIN 53380
Melt Flow3.45 g/10 min3.45 g/10 min 190°C/2.16 kg; ISO 1133

Mechanical Properties
Elongation at BreakMin 50 %Min 50 % 50 mm/min; Nominal; ISO 527

Thermal Properties
Melting Point112 °C234 °F 10 K/min

Optical Properties
Transmission, Visible82 %82 % ASTM D1003

Descriptive Properties
ColorTransparent 
Commercial Status (March 2007)North America and Europe 
Impact ModifiedNo 
Primary Processing TechniqueBlown Film 
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。