BASF Ultraform N 2310 P Q600 Acetal

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Acetal; Polymer; Thermoplastic

Material Notes:
Information provided by BASF Corporation.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesMetricEnglishComments
Density1.4 g/cc0.0506 lb/in³ ISO 1183
Water Absorption0.8 %0.8 % ISO 62
Moisture Absorption at Equilibrium0.2 %0.2 % 23°C/50% R.H.; ISO 62
Linear Mold Shrinkage0.02 cm/cm0.02 in/in MD; ASTM Test
Linear Mold Shrinkage0.021 cm/cm0.021 in/in ISO Data; Parallel to Flow
Linear Mold Shrinkage, Transverse0.021 cm/cm0.021 in/in ISO Data
Melt Flow7.5 g/10 min7.5 g/10 min 190°C/2.16 kg; ISO 1133

Mechanical Properties
Hardness, Rockwell R8585 ASTM D785
Tensile Strength, Yield61 MPa8850 psi 50 mm/min; ISO 527
Tensile Strength, Yield61 MPa8850 psi 2 in/min; ASTM D638
Elongation at Break30 %30 % 50 mm/min; Nominal; ISO 527
Elongation at Yield10 %10 % 2 in/min; ASTM D638
Elongation at Yield10 %10 % 50 mm/min; ISO 527
Tensile Modulus2.6 GPa377 ksi ASTM D638
Tensile Modulus2.6 GPa377 ksi 1 mm/min; ISO 527
Flexural Modulus2.34 GPa339 ksi ASTM D790
Charpy Impact Unnotched20 J/cm²95.2 ft-lb/in² ISO 179
Charpy Impact, Unnotched Low Temp18 J/cm²85.7 ft-lb/in² at -30°C; ISO 179
Charpy Impact, Notched0.55 J/cm²2.62 ft-lb/in² ISO 179
Tensile Creep Modulus, 1 hour1900 MPa276000 psi ISO 899
Tensile Creep Modulus, 1000 hours1300 MPa189000 psi ISO 899
Izod Impact, Notched @ -40°C0.55 J/cm1.03 ft-lb/in ASTM D256
Izod Impact, Notched0.00641 J/cm0.012 ft-lb/in ASTM D256

Electrical Properties
Volume Resistivity1e+012 ohm-cm1e+012 ohm-cm IEC 60093
Surface Resistance1e+012 ohm1e+012 ohm IEC 60093
Dielectric Constant3.83.8 1 MHz; IEC 60250
Dielectric Constant3.83.8 100 Hz; IEC 60250
Dielectric Strength40 kV/mm1020 kV/in IEC 60243-1
Dissipation Factor0.0010.001 100 Hz; IEC 60250
Dissipation Factor0.0050.005 1 MHz; IEC 60250
Comparative Tracking Index600 V600 V IEC 60112

Thermal Properties
CTE, linear 20°C110 µm/m-°C61.1 µin/in-°F Parallel; ISO 11359
CTE, linear 20°C60 µm/m-°C33.3 µin/in-°F ASTM E831
Melting Point166 °C331 °F ASTM D3418
Melting Point166 °C331 °F 10 K/min
Deflection Temperature at 0.46 MPa (66 psi)154 °C309 °F ASTM D648
Deflection Temperature at 0.46 MPa (66 psi)95 °C203 °F ISO 75
Deflection Temperature at 1.8 MPa (264 psi)105 °C221 °F ISO 75
Deflection Temperature at 1.8 MPa (264 psi)99 °C210 °F ASTM D648
Vicat Softening Point150 °C302 °F (50 °C/h / 50N) - B/50; ISO 306
Flammability, UL94HBHB .75 mm
Oxygen Index15 %15 % ISO 4589-1/-2

Descriptive Properties
ColorNatural 
Commercial Status (March 2007)Active America 
Impact ModifiedNo 
Primary Processing TechniqueInjection Molding 
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。