Arkema Group RILSAN® Fine Powders Polyamide 11
Subcategory: Nylon; Nylon 11; Polymer; Thermoplastic
Material Notes: Rilsan® fine powder coatings offer weatherability, long-lasting adhesion, chalk resistance, chemical resistance to aliphatic hydrocarbons, bases, salt solutions, oils, greases and other petroleum products. Typical Applications:- Shopping carts
- Dishwasher baskets
- Hand mixers
- File rods
- Wire shelves
Information provided by Arkema Group
Mechanical Properties | Metric | English | Comments |
|
Tensile Strength, Ultimate | 38 - 47 MPa | 5510 - 6820 psi | |
Taber Abrasion, mg/1000 Cycles | 17 | 17 | CS 17 wheel, 1 kg load |
Electrical Properties |
|
Volume Resistivity | 3.5e+014 ohm-cm | 3.5e+014 ohm-cm | 20°C and 65% RH at 500 V; ASTM D257 |
Surface Resistance | 2.4e+014 ohm | 2.4e+014 ohm | 20°C and 65% RH at 500 V; ASTM D257 |
Dielectric Constant | 3.1 | 3.1 | 1 MHz |
Dielectric Constant, Low Frequency | 3.9 | 3.9 | 100 Hz |
Dielectric Strength | 30.5 kV/mm | 775 kV/in | 0.4 mm thick |
Thermal Properties |
|
Heat of Fusion | 83.7 J/g | 36 BTU/lb | |
CTE, linear 20°C | 150 µm/m-°C | 83.3 µin/in-°F | |
Descriptive Properties | |
Flammability | self-extinguishing | ASTM D 635 (measured at a thickness greater than 3mm to eliminate the influence of substrate) |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|