Arkema Rilsan® Powder D40 Natural Nylon 11, Coating Grade
Subcategory: Nylon; Nylon 11; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA11; Polyamide 11
Material Notes: Powder D40 NATURAL - RILSAN POLYAMIDE 11 (PA11) POWDER Unpigmented and clear Powder as an additive for paints. Improves the scratch and abrasion resistance of paints. Allows for different texture depending on the granulometry used. Can be dispersed completely in liquid media. Excellent chemical resistance. The range includes several colors. The properties listed in the data base have been measured on a corresponding RILSAN PA11 Granule. ISO data provided by the manufacturer, Arkema.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Metric | English | Comments |
|
Density | 1.04 g/cc | 0.0376 lb/in³ | |
Water Absorption | 1.9 % | 1.9 % | |
Electrical Properties |
|
Electrical Resistivity | 1e+014 ohm-cm | 1e+014 ohm-cm | |
Surface Resistance | 1e+014 ohm | 1e+014 ohm | |
Dielectric Strength | 30 kV/mm | 762 kV/in | |
Thermal Properties |
|
Melting Point | 185 °C | 365 °F | 10°C/min |
Vicat Softening Point | 160 °C | 320 °F | 50°C/hr; 50N |
Flammability, UL94 | HB | HB | 1.6 mm |
Flammability, UL94 | V-2 | V-2 | 3.2 mm |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|