COMSOL CD

Arkema Rilsan® Powder ESY Black X 7260 Nylon 11, Coating Grade

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Nylon; Nylon 11; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA11; Polyamide 11

Material Notes:
Powder ESY BLACK X 7260 - RILSAN POLYAMIDE 11 (PA11) POWDER

Melt mix black powder for coating of metallic parts by electrostatic spray, and post fused in an oven.

There is a wide range of colors.

The properties listed in the data base have been measured on a corresponding RILSAN PA11 Granule.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesMetricEnglishComments
Density1.35 g/cc0.0488 lb/in³ 
Water Absorption1.9 %1.9 % 

Electrical Properties
Electrical Resistivity1e+014 ohm-cm1e+014 ohm-cm 
Surface Resistance1e+014 ohm1e+014 ohm 
Dielectric Strength30 kV/mm762 kV/in 

Thermal Properties
Melting Point185 °C365 °F 10°C/min
Vicat Softening Point160 °C320 °F 50°C/hr; 50N
Flammability, UL94HBHB 1.6 mm
Flammability, UL94V-2V-2 3.2 mm
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。