Arkema Rilsan® AESN G9 T6L Nylon 12, Graphite Filled (Conditioned)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12,EHLS,22-010,CD10 Rigid grade with graphite fillers for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents. Very low friction coefficient. No need of lubricant. Excellent wear and chemical resistance. Long service life. Example applications: Control cables tubing, parking brake control cable, cable for opening doors. ISO data provided by the manufacturer, Arkema.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Metric | English | Comments |
|
Density | 1.07 g/cc | 0.0387 lb/in³ | |
Melt Flow | 2.1 g/10 min | 2.1 g/10 min | 235°C/2.16 kg load |
Mechanical Properties |
|
Tensile Strength, Yield | 45 MPa | 6530 psi | 50 mm/min |
Elongation at Break | Min 50 % | Min 50 % | Nominal Strain; 50 mm/min |
Elongation at Yield | 7 % | 7 % | 50 mm/min |
Tensile Modulus | 2.2 GPa | 319 ksi | 1 mm/min |
Charpy Impact Unnotched | 13.3 J/cm² | 63.3 ft-lb/in² | |
Charpy Impact, Notched, Low Temp | 0.42 J/cm² | 2 ft-lb/in² | at -30°C |
Charpy Impact, Unnotched Low Temp | 11.1 J/cm² | 52.8 ft-lb/in² | at -30°C |
Charpy Impact, Notched | 0.45 J/cm² | 2.14 ft-lb/in² | |
Electrical Properties |
|
Electrical Resistivity | 1e+014 ohm-cm | 1e+014 ohm-cm | |
Surface Resistance | 1e+014 ohm | 1e+014 ohm | |
Thermal Properties |
|
CTE, linear 20°C | 80 µm/m-°C | 44.4 µin/in-°F | Parallel to flow |
Melting Point | 174 °C | 345 °F | (Dry) |
Deflection Temperature at 0.46 MPa (66 psi) | 162 °C | 324 °F | |
Deflection Temperature at 1.8 MPa (264 psi) | 65 °C | 149 °F | |
Flammability, UL94 | V-2 | V-2 | 3.2 mm |
Flammability, UL94 | V-2 | V-2 | 1.6 mm |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|