Arkema Rilsan® AESN TL Nylon 12, Flexible Tubing Grade (Dry)
Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12,EHL,22-010 Rigid grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized. High impact strength. Good chemical resistance. Very good ability to be processed at high speed. Example applications: For general use. ISO data provided by the manufacturer, Arkema.
Physical Properties | Metric | English | Comments |
|
Density | 1.01 g/cc | 0.0365 lb/in³ | |
Water Absorption | 1.6 % | 1.6 % | |
Melt Flow | 2.5 g/10 min | 2.5 g/10 min | 235°C/2.16 kg load |
Mechanical Properties |
|
Tensile Strength, Yield | 48 MPa | 6960 psi | 50 mm/min |
Elongation at Break | Min 50 % | Min 50 % | Nominal Strain; 50 mm/min |
Elongation at Yield | 5 % | 5 % | 50 mm/min |
Tensile Modulus | 1.69 GPa | 245 ksi | 1 mm/min |
Thermal Properties |
|
Melting Point | 174 °C | 345 °F | 10°C/min |
Flammability, UL94 | HB | HB | 1.6 mm |
Flammability, UL94 | V-2 | V-2 | 3.2 mm |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|