Arkema Rilsan® AMN D Nylon 12, Rigid, Injection Grade (Conditioned)
Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12,MR,14-010 Rigid grade for injection molding. Available colors: black, natural, orange, red and white. Possibilities of heat and light stabilizing agents. Mold-release agent. Good mechanical properties. Low friction coefficient. Easy filling of the mold due to its well adapted melt viscosity. Low shrinkage: include 1% on average for the design of the mold. Very good dimensional stability (low moisture absorption). High rate of production. UL classification: UL94 V2 (3,05mm) RTI(C) 65/65/65 Example applications: Stressed mechanical parts in all industrial field. ISO data provided by the manufacturer, Arkema.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Metric | English | Comments |
|
Density | 1.01 g/cc | 0.0365 lb/in³ | |
Melt Flow | 69.4 g/10 min | 69.4 g/10 min | 235°C/2.16 kg load |
Mechanical Properties |
|
Tensile Strength, Yield | 39 MPa | 5660 psi | 50 mm/min |
Elongation at Break | Min 50 % | Min 50 % | Nominal Strain; 50 mm/min |
Elongation at Yield | 10 % | 10 % | 50 mm/min |
Tensile Modulus | 1.17 GPa | 170 ksi | 1 mm/min |
Charpy Impact Unnotched | NB | NB | |
Charpy Impact, Notched, Low Temp | 0.59 J/cm² | 2.81 ft-lb/in² | at -30°C |
Charpy Impact, Unnotched Low Temp | NB | NB | |
Charpy Impact, Notched | 0.61 J/cm² | 2.9 ft-lb/in² | |
Electrical Properties |
|
Electrical Resistivity | 1e+014 ohm-cm | 1e+014 ohm-cm | |
Surface Resistance | 1e+014 ohm | 1e+014 ohm | |
Dielectric Strength | 30 kV/mm | 762 kV/in | |
Comparative Tracking Index | 600 V | 600 V | |
Thermal Properties |
|
CTE, linear 20°C | 130 µm/m-°C | 72.2 µin/in-°F | Parallel to flow |
CTE, linear 20°C Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | |
Melting Point | 174 °C | 345 °F | (Dry) |
Deflection Temperature at 0.46 MPa (66 psi) | 135 °C | 275 °F | |
Deflection Temperature at 1.8 MPa (264 psi) | 55 °C | 131 °F | |
Vicat Softening Point | 142 °C | 288 °F | 50°C/hr; 50N |
Flammability, UL94 | HB | HB | 1.6 mm |
Flammability, UL94 | V-2 | V-2 | 3.2 mm |
Oxygen Index | 21 % | 21 % | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|