Arkema Rilsan® AMN P20 TLD Nylon 12, Flexible, Injection Grade (Conditioned)
Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12-P,MHLR,14-005 Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent. Good impact strength. Flexibility and dynamic properties. Easy filling of the mold due to its well adapted viscosity. Low shrinkage: include 1% on average for the design of the mold. Good dimensional stability (low moisture absorption). Example applications: Flexible parts with high impact strength and vibration resistance. ISO data provided by the manufacturer, Arkema.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Metric | English | Comments |
|
Density | 1.02 g/cc | 0.0368 lb/in³ | |
Melt Flow | 42 g/10 min | 42 g/10 min | 235°C/2.16 kg load |
Mechanical Properties |
|
Tensile Strength, Yield | 31 MPa | 4500 psi | 50 mm/min |
Elongation at Break | Min 50 % | Min 50 % | Nominal Strain; 50 mm/min |
Elongation at Yield | 19 % | 19 % | 50 mm/min |
Tensile Modulus | 0.57 GPa | 82.7 ksi | 1 mm/min |
Charpy Impact Unnotched | NB | NB | |
Charpy Impact, Notched, Low Temp | 0.41 J/cm² | 1.95 ft-lb/in² | at -30°C |
Charpy Impact, Unnotched Low Temp | NB | NB | |
Charpy Impact, Notched | 1.77 J/cm² | 8.42 ft-lb/in² | |
Electrical Properties |
|
Electrical Resistivity | 1e+012 ohm-cm | 1e+012 ohm-cm | |
Surface Resistance | 1e+012 ohm | 1e+012 ohm | |
Dielectric Strength | 26 kV/mm | 660 kV/in | |
Comparative Tracking Index | 600 V | 600 V | |
Thermal Properties |
|
CTE, linear 20°C | 120 µm/m-°C | 66.7 µin/in-°F | Parallel to flow |
Melting Point | 174 °C | 345 °F | (Dry) |
Deflection Temperature at 0.46 MPa (66 psi) | 130 °C | 266 °F | |
Deflection Temperature at 1.8 MPa (264 psi) | 48 °C | 118 °F | |
Vicat Softening Point | 134 °C | 273 °F | 50°C/hr; 50N |
Flammability, UL94 | HB | HB | 1.6 mm |
Flammability, UL94 | HB | HB | 3.1 mm |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.

|