NetComposites

Arkema Rilsan® AMN Y TLD Nylon 12, MoS2 Filled (Conditioned)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12,MHLS,14-010,MD05

Grade with molybdenum filler for injection molding. Available color: steel gray. Light and heat stabilized. Mold-release agent.

Low friction coefficient. Good impact strength. Easy filling of the mold due to its well adapted viscosity. Low shrinkage: include 1% on average for the design of the mold. Very good dimensional stability (low moisture absorption).

Example applications: Moving mechanical parts such as gear.

ISO data provided by the manufacturer, Arkema.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesMetricEnglishComments
Density1.02 g/cc0.0368 lb/in³ 
Melt Flow50 g/10 min50 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Yield39 MPa5660 psi 50 mm/min
Elongation at BreakMin 50 %Min 50 % Nominal Strain; 50 mm/min
Elongation at Yield12 %12 % 50 mm/min
Tensile Modulus1.38 GPa200 ksi 1 mm/min

Electrical Properties
Electrical Resistivity1e+014 ohm-cm1e+014 ohm-cm 
Surface Resistance1e+014 ohm1e+014 ohm 
Dielectric Strength55 kV/mm1400 kV/in 
Comparative Tracking Index600 V600 V 

Thermal Properties
CTE, linear 20°C90 µm/m-°C50 µin/in-°F Parallel to flow
Melting Point174 °C345 °F (Dry)
Deflection Temperature at 0.46 MPa (66 psi)143 °C289 °F 
Deflection Temperature at 1.8 MPa (264 psi)65 °C149 °F 
Vicat Softening Point145 °C293 °F 50°C/hr; 50N
Flammability, UL94HBHB 1.6 mm
Flammability, UL94V-2V-2 3.2 mm
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。