Arkema Rilsan® AUM 30 T6LD Nylon 12, 30% Glass Bead Filled (Conditioned)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12,MHLR,16-020,GB30

Rigid grad with glass beads filler (30%) for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.

Reinforced isotropic performances. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. High dimensional stability (low moisture absorption). Low coefficient of linear expansion.

Example applications: Mechanical parts with dimensional precision.

ISO data provided by the manufacturer, Arkema.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesMetricEnglishComments
Density1.22 g/cc0.0441 lb/in³ 
Melt Flow70.8 g/10 min70.8 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Yield39 MPa5660 psi 50 mm/min
Elongation at Break32 %32 % Nominal Strain; 50 mm/min
Elongation at Yield6 %6 % 50 mm/min
Tensile Modulus1.72 GPa249 ksi 1 mm/min
Charpy Impact Unnotched4.72 J/cm²22.5 ft-lb/in² 
Charpy Impact, Notched, Low Temp0.45 J/cm²2.14 ft-lb/in² at -30°C
Charpy Impact, Unnotched Low Temp4.95 J/cm²23.6 ft-lb/in² at -30°C
Charpy Impact, Notched0.56 J/cm²2.67 ft-lb/in² 

Electrical Properties
Electrical Resistivity1e+013 ohm-cm1e+013 ohm-cm 
Surface Resistance1e+013 ohm1e+013 ohm 
Dielectric Strength40 kV/mm1020 kV/in 
Comparative Tracking Index600 V600 V 

Thermal Properties
CTE, linear 20°C70 µm/m-°C38.9 µin/in-°F Parallel to flow
Melting Point174 °C345 °F (Dry)
Deflection Temperature at 0.46 MPa (66 psi)155 °C311 °F 
Deflection Temperature at 1.8 MPa (264 psi)60 °C140 °F 
Vicat Softening Point160 °C320 °F 50°C/hr; 50N
Flammability, UL94HBHB 3.1 mm
Flammability, UL94HBHB 1.6 mm
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。