Arkema Rilsan® AUM 50 NOIR T6LD Nylon 12, 50% Glass Bead Filled (Conditioned)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12,MHLR,16-020,GB50 Rigid grad with glass beads filler (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agents. Mold-release agent. Good mechanical properties. Reinforced isotropic performances. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. High dimensional stability (low moisture absorption). Low coefficient of linear expansion. Potable water contact approval WRC 950 1509. Example applications: Mechanical parts with dimensional precision. ISO data provided by the manufacturer, Arkema.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Metric | English | Comments |
|
Density | 1.42 g/cc | 0.0513 lb/in³ | |
Melt Flow | 5 g/10 min | 5 g/10 min | 235°C/2.16 kg load |
Mechanical Properties |
|
Tensile Strength, Yield | 49 MPa | 7110 psi | 50 mm/min |
Elongation at Break | 18 % | 18 % | Nominal Strain; 50 mm/min |
Elongation at Yield | 5 % | 5 % | 50 mm/min |
Tensile Modulus | 3.13 GPa | 454 ksi | 1 mm/min |
Charpy Impact Unnotched | 8.01 J/cm² | 38.1 ft-lb/in² | |
Charpy Impact, Notched, Low Temp | 0.38 J/cm² | 1.81 ft-lb/in² | at -30°C |
Charpy Impact, Unnotched Low Temp | 6.11 J/cm² | 29.1 ft-lb/in² | at -30°C |
Charpy Impact, Notched | 0.44 J/cm² | 2.09 ft-lb/in² | |
Electrical Properties |
|
Electrical Resistivity | 1e+013 ohm-cm | 1e+013 ohm-cm | |
Surface Resistance | 1e+013 ohm | 1e+013 ohm | |
Dielectric Strength | 40 kV/mm | 1020 kV/in | |
Comparative Tracking Index | 600 V | 600 V | |
Thermal Properties |
|
CTE, linear 20°C | 60 µm/m-°C | 33.3 µin/in-°F | Parallel to flow |
Melting Point | 174 °C | 345 °F | (Dry) |
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | |
Deflection Temperature at 1.8 MPa (264 psi) | 68 °C | 154 °F | |
Vicat Softening Point | 165 °C | 329 °F | 50°C/hr; 50N |
Flammability, UL94 | HB | HB | 3.1 mm |
Flammability, UL94 | HB | HB | 1.6 mm |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|