Arkema Rilsan® AZM 30 GT8LD Nylon 12, 30% Glass Fiber Filled (Dry)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12,MHLS,16-050,(G+C)(F+D)(30+05)

Rigid grade with glass fiber (30%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stabilizing agent. Mold-release agent.

High rigidity. Low friction coefficient. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. Low coefficient of linear expansion. High dimensional stability.

Example applications: Mechanical parts with friction such as knuckle joint for windshield wiper.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesMetricEnglishComments
Density1.23 g/cc0.0444 lb/in³ 
Melt Flow2.2 g/10 min2.2 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Ultimate114 MPa16500 psi 5 mm/min
Elongation at Break6 %6 % 5 mm/min
Tensile Modulus8.75 GPa1270 ksi 1 mm/min
Charpy Impact Unnotched9.3 J/cm²44.3 ft-lb/in² 
Charpy Impact, Notched, Low Temp1.35 J/cm²6.42 ft-lb/in² at -30°C
Charpy Impact, Unnotched Low Temp9.11 J/cm²43.4 ft-lb/in² at -30°C
Charpy Impact, Notched1.77 J/cm²8.42 ft-lb/in² 

Electrical Properties
Dissipation Factor0.000360.00036 1 MHz
Dissipation Factor, Low Frequency0.000450.00045 100 Hz

Thermal Properties
Melting Point174 °C345 °F 10°C/min
Flammability, UL94HBHB 3.1 mm
Flammability, UL94HBHB 1.6 mm
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。