Arkema Rilsan® MA 4420 Nylon 12, Flexible Tubing Grade (Dry)
Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA11; Polyamide 11
Material Notes: Designation ISO 1874-PA12-HI,EHL,22-003 Flexible grade for tubes extrusion. Available color: black. Light and heat stabilized. Flexibility. High burst pressure and impact strength. Fit for use in a wide range of temperature. Very good chemical resistance. Example applications: Tubes for air brake system in trucks approved by ISO 7628, DIN 73378 (PA12-PHLY), NFR 12632, SAEJ 844. ISO data provided by the manufacturer, Arkema.
Physical Properties | Metric | English | Comments |
|
Water Absorption | 1.2 % | 1.2 % | |
Moisture Absorption at Equilibrium | 0.55 % | 0.55 % | Humidity Absorption |
Melt Flow | 4.8 g/10 min | 4.8 g/10 min | 235°C/2.16 kg load |
Mechanical Properties |
|
Tensile Strength, Yield | 33 MPa | 4790 psi | 50 mm/min |
Elongation at Break | Min 50 % | Min 50 % | Nominal Strain; 50 mm/min |
Elongation at Yield | 19 % | 19 % | 50 mm/min |
Tensile Modulus | 0.72 GPa | 104 ksi | 1 mm/min |
Charpy Impact Unnotched | NB | NB | |
Charpy Impact, Notched, Low Temp | 0.43 J/cm² | 2.05 ft-lb/in² | at -30°C |
Charpy Impact, Unnotched Low Temp | NB | NB | |
Charpy Impact, Notched | 1.6 J/cm² | 7.61 ft-lb/in² | |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 42 °C | 108 °F | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|