LANXESS Pocan® KU 2-7426 PET
Subcategory: Filled/Reinforced Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polymer; Thermoplastic
Close Analogs: LANXESS was spun-off from Bayer in early 2005.
Material Notes: Key Features: Suitable processing methods: Information provided by Bayer Polymers.
| Physical Properties | Metric | English | Comments |
|
| Density | 1.55 g/cc | 0.056 lb/in³ | |
| Water Absorption | 0.3 % | 0.3 % | |
| Moisture Absorption at Equilibrium | 0.1 % | 0.1 % | 23°C/50% R.H. |
| Melt Flow | 35 g/10 min | 35 g/10 min | (cm³/10 min.) 260°C/2.16 kg |
Mechanical Properties |
|
| Tensile Strength, Ultimate | 130 MPa | 18900 psi | |
| Elongation at Break | 2 % | 2 % | |
| Tensile Modulus | 9.6 GPa | 1390 ksi | |
Thermal Properties |
|
| Melting Point | 250 °C | 482 °F | 10°C/min |
| Vicat Softening Point | 235 °C | 455 °F | 50°C/h 50N |
| Flammability, UL94 | V-2 | V-2 | 1.6 mm |
Processing Properties |
|
| Melt Temperature | 270 °C | 518 °F | Injection Molding |
| Mold Temperature | 130 °C | 266 °F | Injection Molding |
| Injection Velocity | 200 mm/sec | 7.87 in/sec | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|