Physical Properties | Metric | English | Comments |
|
Density | 1.2 g/cc | 0.0434 lb/in³ | |
Mechanical Properties |
|
Tensile Strength, Yield | 5 MPa | 725 psi | Stress at 50% Strain |
Elongation at Break | Min 50 % | Min 50 % | |
Electrical Properties |
|
Volume Resistivity | 8e+009 ohm-cm | 8e+009 ohm-cm | |
Surface Resistance | 5e+011 ohm | 5e+011 ohm | |
Dielectric Constant | 5.6 | 5.6 | 1 MHz |
Dielectric Constant | 6.5 | 6.5 | 100 Hz |
Dielectric Strength | 17.5 kV/mm | 445 kV/in | |
Dissipation Factor | 0.025 | 0.025 | 100 Hz |
Dissipation Factor | 0.06 | 0.06 | 1 MHz |
Thermal Properties |
|
CTE, linear 20°C | 150 µm/m-°C | 83.3 µin/in-°F | Parallel |
Vicat Softening Point | 91 °C | 196 °F | 50°C/h 50N |
Glass Temperature | -42 °C | -43.6 °F | 10°C/min |
Flammability, UL94 | HB | HB | 1.5 mm UL Recognized |
Flammability, UL94 | V-2 | V-2 | 3 mm UL Recognized |
Processing Properties |
|
Melt Temperature | 200 °C | 392 °F | Injection Molding |
Mold Temperature | 30 °C | 86 °F | Injection Molding |
Injection Pressure | 45 MPa | 6530 psi | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|