![COMSOL CD](/images/COMSOL600x60.gif)
Bayer MaterialScience Texin® 4215 Urethane Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic
Key Words: TPU
Material Notes: Key Features: Suitable processing methods: - Injection molding
- Film extrusion
- Profile extrusion
- Sheet extrusion
Information provided by Bayer Polymers.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Metric | English | Comments |
|
Density | 1.21 g/cc | 0.0437 lb/in³ | |
Mechanical Properties |
|
Tensile Strength, Yield | 21 MPa | 3050 psi | Stress at 50% Strain |
Elongation at Break | Min 50 % | Min 50 % | |
Thermal Properties |
|
CTE, linear 20°C | 115 µm/m-°C | 63.9 µin/in-°F | Parallel |
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | |
Deflection Temperature at 1.8 MPa (264 psi) | 74 °C | 165 °F | |
Vicat Softening Point | 140 °C | 284 °F | 50°C/h 50N |
Glass Temperature | -35 °C | -31 °F | 10°C/min |
Flammability, UL94 | HB | HB | 1.5 mm UL Recognized |
Processing Properties |
|
Melt Temperature | 230 °C | 446 °F | Injection Molding |
Mold Temperature | 35 °C | 95 °F | Injection Molding |
Injection Pressure | 45 MPa | 6530 psi | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
![New MatWeb Services](/images/matweb_premium2.gif)
|