DSM Engineering Plastics Stanyl® TW241F10 (COND) Nylon 46 50% Glass Reinforced, Heat Stabilized (North America)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic
Key Words: Polyamide 46
Material Notes: Information provided by DSM Engineering Plastics.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Metric | English | Comments |
|
Density | 1.62 g/cc | 0.0585 lb/in³ | (DAM); ISO 1183 |
Mechanical Properties |
|
Tensile Strength at Break | 160 MPa | 23200 psi | ISO 527-1/-2 |
Elongation at Break | 5 % | 5 % | ISO 527-1/-2 |
Tensile Modulus | 10 GPa | 1450 ksi | ISO 527-1/-2 |
Charpy Impact Unnotched | 10 J/cm² | 47.6 ft-lb/in² | ISO 179/1eU |
Charpy Impact, Notched, Low Temp | 1.4 J/cm² | 6.66 ft-lb/in² | at -30°C; ISO 179/1eU |
Charpy Impact, Unnotched Low Temp | 8 J/cm² | 38.1 ft-lb/in² | at -30°C; ISO 179/1eU |
Charpy Impact, Notched | 2.4 J/cm² | 11.4 ft-lb/in² | ISO 179/1eU |
Electrical Properties |
|
Volume Resistivity | 1e+008 ohm-cm | 1e+008 ohm-cm | IEC 60093 |
Dielectric Strength | 20 kV/mm | 508 kV/in | IEC 60243-1 |
Comparative Tracking Index | 300 V | 300 V | IEC 60112 |
Thermal Properties |
|
Melting Point | 295 °C | 563 °F | (DAM); ISO 11357-1/-3 |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|