DSM Engineering Plastics Stanyl® TW363 (COND) Nylon 46 Heat Stabilized, Impact Modified (North America)
Subcategory: Nylon; Nylon 46; Polymer; Thermoplastic
Key Words: Polyamide 46
Material Notes: Information provided by DSM Engineering Plastics.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Metric | English | Comments |
|
Density | 1.1 g/cc | 0.0397 lb/in³ | (DAM); ISO 1183 |
Mechanical Properties |
|
Tensile Strength, Yield | 45 MPa | 6530 psi | ISO 527-1/-2 |
Elongation at Yield | Min 50 % | Min 50 % | Nominal Strain at Yield; ISO 527-1/-2 |
Tensile Modulus | 0.6 GPa | 87 ksi | ISO 527-1/-2 |
Charpy Impact Unnotched | NB | NB | ISO 179/1eU |
Charpy Impact, Notched, Low Temp | 3 J/cm² | 14.3 ft-lb/in² | at -30°C; ISO 179/1eU |
Charpy Impact, Unnotched Low Temp | NB | NB | at -30°C; ISO 179/1eU |
Charpy Impact, Notched | 12.5 J/cm² | 59.5 ft-lb/in² | ISO 179/1eU |
Electrical Properties |
|
Volume Resistivity | 1e+007 ohm-cm | 1e+007 ohm-cm | IEC 60093 |
Dielectric Strength | 15 kV/mm | 381 kV/in | IEC 60243-1 |
Comparative Tracking Index | 475 V | 475 V | IEC 60112 |
Thermal Properties |
|
Melting Point | 295 °C | 563 °F | (DAM); ISO 11357-1/-3 |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|