MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

COMSOL CD

DSM Arnitel® PL581 58 Shore D, Injection Grade Copolyester Elastomer (North America)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Elastomer, TPE; Polyester TPE; Polymer; Thermoplastic

Material Notes:
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.

Arnitel does not require vulcanization. This leads to substantial reductions in part cost. Arnitel can be used over a wide range of temperatures. Arnitel has exceptional fatigue, creep resistance and resistance to oils, greases and many other chemicals.

Characteristics of Arnitel:

  • Excellent strength over a wide range of temperatures
  • Excellent dynamic properties e.g. creep and fatigue
  • High heat resistance
  • Exceptional resistance to oils and greases
  • Good chemical resistance
  • High degree of versatility in processing
  • Easy coloring using masterbatches
  • Surface quality from high gloss to textured
  • Excellent heat resistance (long term 165°C)
  • Good electrical insulation properties
  • Low moisture absorption, excellent dimensional stability
  • Easy flow, fast cooling times

Typical Applications:

  • Automotive: Arnitel® is extensively used in the automotive industry for applications requiring exceptional fatigue resistance and resistance to oil and greases. Examples are: Rack and Pinion Bellows, Constant Velocity Joint Boots (CVJ Boots), Air brake tubings.
  • Arnitel in the Electronic and Consumer Goods Industry: Arnitel® finds enormous potential and is also widely used in the consumer electronics by some of the world's best companies. Arnitel® is the best choice for low noise gears where their exceptional processability without any defects such as flash, makes it the material solution of choice. Arnitel® is also used in highly demanding applications such as in mobile phone antennas.

Arnitel® has exceptional flexibility and can perform or even outperform functions that normally require conventional rubbers. Available in a wide range of hardnesses, Arnitel can replace metals, thermoplastics, leather and rubber, often with a reduction in finished part costs.

Information provided by DSM.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesMetricEnglishComments
Density1.23 g/cc0.0444 lb/in³ ISO 1183
Water Absorption2.5 %2.5 % Sim. to ISO 62
Moisture Absorption at Equilibrium0.4 %0.4 % Humidity Absorption; Sim. to ISO 62
Melt Flow13.53 g/10 min13.53 g/10 min Calculated from Volume Flow Rate of 11 cm3/10 min, 2.16 kg, 230°C; ISO 1133

Mechanical Properties
Hardness, Shore D5555 3 s; ISO 868
Tensile Strength, Yield10 MPa1450 psi Stress at 5% Strain; ISO 527-1/-2
Tensile Strength, Yield13.7 MPa1990 psi Stress at 10% Strain; ISO 527-1/-2
Tensile Strength, Yield16.8 MPa2440 psi Stress at 50% Strain; ISO 527-1/-2
Tensile Strength, Yield18.5 MPa2680 psi Stress at 100% Strain; ISO 527-1/-2
Elongation at Break300 %300 % ISO 527-1/-2
Tensile Modulus0.3 GPa43.5 ksi ISO 527-1/-2
Izod Impact, Notched (ISO)NBNB 23°C; ISO 180/1A
Charpy Impact, Notched, Low Temp1.6 J/cm²7.61 ft-lb/in² -30°C; ISO 179/1eA
Charpy Impact, NotchedNBNB 23°C; ISO 179/1eA

Electrical Properties
Volume ResistivityMin 1e+015 ohm-cmMin 1e+015 ohm-cm IEC 60093
Surface Resistance1e+014 ohm1e+014 ohm IEC 60093
Dielectric Constant44 1 MHz; IEC 60250
Dielectric Strength21 kV/mm533 kV/in IEC 60243-1
Dissipation Factor0.040.04 1 MHz; IEC 60250
Comparative Tracking Index600 V600 V IEC 60112

Thermal Properties
CTE, linear 20°C110 µm/m-°C61.1 µin/in-°F Parallel; ISO 11359-1/-2
CTE, linear 20°C Transverse to Flow110 µm/m-°C61.1 µin/in-°F Normal; ISO 11359-1/-2
Melting Point218 °C424 °F 10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi)100 °C212 °F ISO 75-1/-2
Vicat Softening Point105 °C221 °F 50°C/h 50N; ISO 306
Vicat Softening Point205 °C401 °F 50°C/h 10N; ISO 306
Flammability, UL94HBHB 1.6 mm nominal thickness; IEC 60695-11-10

Descriptive Properties
High impact or impact modifiedYes 
Injection MoldingYes 
Other ExtrusionYes 
Without fillersYes 
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。