DSM Stanyl® TW275F6 Nylon 46-30% Glass Reinforced, Heat Stabilized, Wear and Friction Modified (Asian Grade) (Dry)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic
Material Notes: Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:- Highest mechanical properties at high temperatures
- Excellent resistance to wear and low friction
- Outstanding flow for easy processing and exceptional design freedom
- Stanyl High Flowgrades that match the best flowing LCPs while maintaining a high level of mechanical properties
Key Applications: Automotive: Powertrain components, Charge-air coolers, EPS and ETC gears, Motor Sensors, Auto connectors, Chain tensionersE&E: Connectors, Microswitches, Bobbins, Memory modules, Motor components, Industrial, Specialty films and fibers, Consumer appliancesInformation provided by DSM.
Physical Properties | Metric | English | Comments |
|
Density | 1.43 g/cc | 0.0517 lb/in³ | ISO 1183 |
Moisture Absorption at Equilibrium | 2.6 % | 2.6 % | Similar to ISO 62 |
Mechanical Properties |
|
Tensile Strength at Break | 205 MPa | 29700 psi | ISO 527-1/-2 |
Elongation at Break | 3.5 % | 3.5 % | ISO 527-1/-2 |
Flexural Modulus | 9 GPa | 1310 ksi | ISO 178 |
Izod Impact, Notched (ISO) | 9 kJ/m² | 4.28 ft-lb/in² | At 23°C; ISO 180/1A |
Izod Impact, Notched, Low Temp (ISO) | 8 kJ/m² | 3.81 ft-lb/in² | At -40°C; ISO 180/1A |
Thermal Properties |
|
CTE, linear 20°C | 20 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
CTE, linear 20°C Transverse to Flow | 80 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
Deflection Temperature at 1.8 MPa (264 psi) | 285 °C | 545 °F | ISO 75-1/-2 |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|