MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Free Trade Publications, Click Here!

DSM Stanyl® TW241F6 Nylon 46-30% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Dry)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic

Material Notes:
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:

  • Highest mechanical properties at high temperatures
  • Excellent resistance to wear and low friction
  • Outstanding flow for easy processing and exceptional design freedom
  • Stanyl High Flowgrades that match the best flowing LCPs while maintaining a high level of mechanical properties

Key Applications:

  • Automotive: Powertrain components, Charge-air coolers, EPS and ETC gears, Motor Sensors, Auto connectors, Chain tensioners
  • E&E: Connectors, Microswitches, Bobbins, Memory modules, Motor components, Industrial, Specialty films and fibers, Consumer appliances

    Information provided by DSM.

    Physical PropertiesMetricEnglishComments
    Density1.41 g/cc0.0509 lb/in³ ISO 1183
    Linear Mold Shrinkage0.005 cm/cm0.005 in/in Parallel; ISO 294-4
    Linear Mold Shrinkage, Transverse0.013 cm/cm0.013 in/in Normal; ISO 194-4

    Mechanical Properties
    Tensile Strength at Break210 MPa30500 psi ISO 527-1/-2
    Elongation at Break4 %4 % ISO 527-1/-2
    Tensile Modulus10 GPa1450 ksi ISO 527-1/-2
    Charpy Impact Unnotched8 J/cm²38.1 ft-lb/in² At 23°C; ISO 179/1eA
    Charpy Impact, Notched, Low Temp1 J/cm²4.76 ft-lb/in² At -30°C; ISO 179/1eA
    Charpy Impact, Unnotched Low Temp7 J/cm²33.3 ft-lb/in² At -30°C; ISO 179/1eA
    Charpy Impact, Notched1.2 J/cm²5.71 ft-lb/in² At 23°C; ISO 179/1eA

    Thermal Properties
    CTE, linear 20°C20 µm/m-°C11.1 µin/in-°F ISO 11359-1/-2
    CTE, linear 20°C Transverse to Flow80 µm/m-°C44.4 µin/in-°F ISO 11359-1/-2
    Melting Point295 °C563 °F 10°C/min; ISO 11357-1/-3
    Deflection Temperature at 1.8 MPa (264 psi)290 °C554 °F ISO 75-1/-2
    Flammability, UL94HBHB 0.75 mm; IEC 60695-11-10
    Printer friendly version Printer friendly version


    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Free Trade Publications, Click Here!

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
  • 请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。