| Physical Properties | Metric | English | Comments |
|
| Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D 792 |
| Density | 1.18 g/cc | 0.0426 lb/in³ | Color; ASTM D 792 |
| Water Absorption | 0.1 % | 0.1 % | 24 hours @ 73F; ASTM D 570 |
| Water Absorption at Saturation | 0.4 % | 0.4 % | Equilibrium, 73F; ASTM D 570 |
| Linear Mold Shrinkage | 0.004 - 0.006 cm/cm | 0.004 - 0.006 in/in | Flow, 0.125 inch; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.004 - 0.006 cm/cm | 0.004 - 0.006 in/in | 0.125 inch; ASTM D 955 |
| Melt Flow | 16 g/10 min | 16 g/10 min | 260C/2.16 kgf; ASTM D 1238 |
Mechanical Properties |
|
| Hardness, Rockwell R | 120 | 120 | ASTM D 785 |
| Tensile Strength @ Yield | 58.6 MPa | 8500 psi | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Break | 50 % | 50 % | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Yield | 5 % | 5 % | Type I, 2.0 in/min; ASTM D 638 |
| Tensile Modulus | 2.69 GPa | 390 ksi | 2.0 in/min; ASTM D 638 |
| Flexural Modulus | 2.69 GPa | 390 ksi | 0.10 in/min, 4" span; ASTM D 790 |
| Flexural Yield Strength | 96.5 MPa | 14000 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Gardner Impact @ 23°C | 58.3 J | 43 ft-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
| Izod Impact, Notched | 4.27 J/cm | 8 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
| Volume Resistivity | 1e+017 ohm-cm | 1e+017 ohm-cm | ASTM D 257 |
| Surface Resistivity per Square | Min 1e+014 ohm | Min 1e+014 ohm | ASTM D 257 |
| Dielectric Constant | 3 | 3 | 100 Hz; ASTM D 150 |
| Dielectric Constant | 3 | 3 | 50 Hz; ASTM D 150 |
| Dielectric Strength | 18 kV/mm | 457 V/mil | in oil, 125 mils; ASTM D 149 |
| Dissipation Factor | 0.0048 | 0.0048 | 50 Hz; ASTM D 150 |
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten (+/- 0.125 inch); PLC Code 6; ASTM D 495 |
| Comparative Tracking Index | 400 - 600 V | 400 - 600 V | (+/- 0.125 inch); PLC Code 1; UL 746A |
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | (+/- 0.125 inch); PLC Code 3; UL 746A |
| High Amp Arc Ignition, HAI | Min 120 arcs | Min 120 arcs | Surface (+/- 0.125 inch); PLC Code 0; UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | 80 - 150 mm/min | 3.15 - 5.91 in/min | (+/- 0.125 inch); PLC Code 3; UL 746A |
Thermal Properties |
|
| CTE, linear 68°F | 72 µm/m-°C | 40 µin/in-°F | Flow, -40F to 140F; ASTM E 831 |
| CTE, linear 68°F, Transverse to Flow | 72 µm/m-°C | 40 µin/in-°F | From -40F to 140F; ASTM E 831 |
| Thermal Conductivity | 0.2 W/m-K | 1.39 BTU-in/hr-ft²-°F | ASTM C 177 |
| Deflection Temperature at 1.8 MPa (264 psi) | 73.9 °C | 165 °F | 0.125 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 80 °C | 176 °F | 0.250 inch, unannealed; ASTM D 648 |
| Vicat Softening Point | 90.6 °C | 195 °F | Rate B; ASTM D 1525 |
| UL RTI, Electrical | 80 °C | 176 °F | UL 746B |
| UL RTI, Mechanical with Impact | 70 °C | 158 °F | UL 746B |
| UL RTI, Mechanical without Impact | 80 °C | 176 °F | UL 746B |
| Flammability, UL94 | V-2 | V-2 | 0.035 in. |
| Flammability, UL94 | V-0 | V-0 | 0.058 in. |
| Flammability, UL94 | 6 | 6 | 0.091 in. |
| Oxygen Index | 35 % | 35 % | ASTM D 2863 |
Descriptive Properties |
|
| CSA File No. | LS88480 | |
| UL File Number, EUROPE | E45329 | |
| UL File Number, GLOBAL | E161759 | |
| UL File Number, USA | E121562 | |
|