SABIC Innovative Plastics CYCOLOY C2801 ABS + Polycarbonate (North America)
Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
| Physical Properties | Metric | English | Comments |
|
| Density | 1.22 g/cc | 0.0441 lb/in³ | ASTM D 792 |
| Linear Mold Shrinkage | 0.004 - 0.005 cm/cm | 0.004 - 0.005 in/in | Flow, 0.125 inch; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.003 - 0.005 cm/cm | 0.003 - 0.005 in/in | 0.125 inch; ASTM D 955 |
Mechanical Properties |
|
| Tensile Strength @ Break | 51.7 MPa | 7500 psi | Type I, 2.0 in/min; ASTM D 638 |
| Tensile Strength @ Yield | 62.1 MPa | 9000 psi | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Break | 110 % | 110 % | Type I, 2.0 in/min; ASTM D 638 |
| Flexural Modulus | 2.72 GPa | 395 ksi | 0.10 in/min, 4" span; ASTM D 790 |
| Flexural Yield Strength | 95.1 MPa | 13800 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Coefficient of Friction | 0.21 | 0.21 | Vs. Steel, Kinetic; ASTM D 1894 |
| Coefficient of Friction, Static | 0.16 | 0.16 | Vs. Steel; ASTM D 1894 |
| K (wear) Factor | 866 x 10-8 mm³/N-M | 430 x 10-10 in³-min/ft-lb-hr | PV = 2000 psi-fpm vs Steel; GE Test |
| Izod Impact, Notched | 1.33 J/cm | 2.5 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
| Comparative Tracking Index | 400 - 600 V | 400 - 600 V | (+/- 0.125 inch); PLC Code 1; UL 746A |
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | (+/- 0.125 inch); PLC Code 3; UL 746A |
| High Amp Arc Ignition, HAI | Min 120 arcs | Min 120 arcs | Surface (+/- 0.125 inch); PLC Code 0; UL 746A |
Thermal Properties |
|
| Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C | 180 °F | 0.250 inch, unannealed; ASTM D 648 |
| UL RTI, Electrical | 60 °C | 140 °F | UL 746B |
| UL RTI, Mechanical with Impact | 60 °C | 140 °F | UL 746B |
| UL RTI, Mechanical without Impact | 60 °C | 140 °F | UL 746B |
| Flammability, UL94 | V-0 | V-0 | 0.059 in. |
| Flammability, UL94 | 6 | 6 | 0.098 in. |
Descriptive Properties | |
| UL File Number, USA | E121562 | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|