SABIC Innovative Plastics CYCOLOY C6600 ABS + Polycarbonate (North America)
Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
| Physical Properties | Metric | English | Comments |
|
| Density | 1.19 g/cc | 0.043 lb/in³ | ASTM D 792 |
| Water Absorption | 0.11 % | 0.11 % | 24 hours @ 73F; ASTM D 570 |
| Linear Mold Shrinkage | 0.004 - 0.006 cm/cm | 0.004 - 0.006 in/in | Flow, 0.125 inch; ASTM D 955 |
| Melt Flow | 21.5 g/10 min | 21.5 g/10 min | 260C/2.16 kgf; ASTM D 1238 |
Mechanical Properties |
|
| Tensile Strength @ Break | 49 MPa | 7100 psi | Type I, 2.0 in/min; ASTM D 638 |
| Tensile Strength @ Yield | 63.4 MPa | 9200 psi | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Break | 80 % | 80 % | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Yield | 4 % | 4 % | Type I, 2.0 in/min; ASTM D 638 |
| Tensile Modulus | 3 GPa | 435 ksi | 2.0 in/min; ASTM D 638 |
| Flexural Modulus | 2.62 GPa | 380 ksi | 0.05 in/min, 2" span; ASTM D 790 |
| Flexural Yield Strength | 94.5 MPa | 13700 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Gardner Impact @ 23°C | 50.8 J | 37.5 ft-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
| Gardner Impact @ 23°C | 50.8 J | 37.5 ft-lb | Instrumented Impact Total Energy, -22F; ASTM D 3763 |
| Izod Impact, Notched | 5.87 J/cm | 11 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
| Volume Resistivity | Min 1e+015 ohm-cm | Min 1e+015 ohm-cm | IEC 60093 |
| Surface Resistivity per Square | Min 1e+015 ohm | Min 1e+015 ohm | IEC 60093 |
| Dielectric Constant | 2.7 | 2.7 | 50 Hz; IEC 60250 |
| Dielectric Constant | 2.7 | 2.7 | 1 MHz; IEC 60250 |
| Dielectric Strength | 17 kV/mm | 432 kV/in | in oil, 3.2 mm; IEC 60243-1 |
| Dissipation Factor | 0.004 | 0.004 | 50 Hz; IEC 60250 |
| Dissipation Factor | 0.006 | 0.006 | 1 MHz; IEC 60250 |
| Comparative Tracking Index | 600 V | 600 V | IEC 112/3rd |
Thermal Properties |
|
| Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | 0.125 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 90 °C | 194 °F | 0.125 inch, unannealed; ASTM D 648 |
| Vicat Softening Point | 99.4 °C | 211 °F | Rate B; ASTM D 1525 |
| UL RTI, Electrical | 80 °C | 176 °F | UL 746B |
| UL RTI, Mechanical with Impact | 70 °C | 158 °F | UL 746B |
| UL RTI, Mechanical without Impact | 80 °C | 176 °F | UL 746B |
| Flammability, UL94 | V-2 | V-2 | 0.03 in. |
| Flammability, UL94 | V-0 | V-0 | 0.059 in. |
| Flammability, UL94 | 6 | 6 | 0.079 in. |
Descriptive Properties | |
| UL File Number, GLOBAL | E161759 | |
| UL File Number, USA | E121562 | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|