SABIC Innovative Plastics CYCOLOY C6800 ABS + Polycarbonate (North America)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesMetricEnglishComments
Density1.18 g/cc0.0426 lb/in³ Color; ASTM D 792
Density1.19 g/cc0.043 lb/in³ ASTM D 792
Water Absorption0.1 %0.1 % 24 hours @ 73F; ASTM D 570
Water Absorption at Saturation0.4 %0.4 % Equilibrium, 73F; ASTM D 570
Linear Mold Shrinkage0.004 - 0.006 cm/cm0.004 - 0.006 in/in Flow, 0.125 inch; ASTM D 955
Linear Mold Shrinkage, Transverse0.004 - 0.006 cm/cm0.004 - 0.006 in/in 0.125 inch; ASTM D 955
Melt Flow11 g/10 min11 g/10 min 260C/2.16 kgf; ASTM D 1238

Mechanical Properties
Hardness, Rockwell R120120 ASTM D 785
Tensile Strength @ Yield62.1 MPa9000 psi Type I, 2.0 in/min; ASTM D 638
Elongation at Break50 %50 % Type I, 2.0 in/min; ASTM D 638
Elongation at Yield5 %5 % Type I, 2.0 in/min; ASTM D 638
Tensile Modulus2.69 GPa390 ksi 2.0 in/min; ASTM D 638
Flexural Modulus2.69 GPa390 ksi 0.05 in/min, 2" span; ASTM D 790
Flexural Yield Strength103 MPa15000 psi 0.05 in/min, 2" span; ASTM D 790
Gardner Impact @ 23°C67.8 J50 ft-lb Instrumented Impact Total Energy, 73°F; ASTM D 3763
Izod Impact, Notched5.87 J/cm11 ft-lb/in 73F; ASTM D 256

Electrical Properties
Volume Resistivity1e+017 ohm-cm1e+017 ohm-cm ASTM D 257
Surface Resistivity per SquareMin 1e+014 ohmMin 1e+014 ohm ASTM D 257
Dielectric Constant33 50 Hz; ASTM D 150
Dielectric Constant33 100 Hz; ASTM D 150
Dielectric Strength18 kV/mm457 V/mil in oil, 125 mils; ASTM D 149
Dissipation Factor0.00480.0048 50 Hz; ASTM D 150
Comparative Tracking IndexMin 600 VMin 600 V (+/- 0.125 inch); PLC Code 0; UL 746A
Hot Wire Ignition, HWI30 - 60 sec30 - 60 sec (+/- 0.125 inch); PLC Code 2; UL 746A
High Amp Arc Ignition, HAIMin 120 arcsMin 120 arcs Surface (+/- 0.125 inch); PLC Code 0; UL 746A

Thermal Properties
CTE, linear 68°F72 µm/m-°C40 µin/in-°F Flow, -40F to 100F; ASTM E 831
CTE, linear 68°F, Transverse to Flow72 µm/m-°C40 µin/in-°F from -40F to 100F; ASTM E 831
Thermal Conductivity0.2 W/m-K1.39 BTU-in/hr-ft²-°F ASTM C 177
Deflection Temperature at 0.46 MPa (66 psi)109 °C229 °F 0.125 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)98.9 °C210 °F 0.125 inch, unannealed; ASTM D 648
UL RTI, Electrical90 °C194 °F UL 746B
UL RTI, Mechanical with Impact85 °C185 °F UL 746B
UL RTI, Mechanical without Impact90 °C194 °F UL 746B
Flammability, UL94V-1V-1 0.058 in.
Flammability, UL94V-0V-0 0.079 in.
Flammability, UL9466 0.102 in.

Descriptive Properties
UL File Number, USAE121562 
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。