SABIC Innovative Plastics CYCOLOY MC1300 ABS + Polycarbonate (North America)
Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
Physical Properties | Metric | English | Comments |
|
Density | 1.1 g/cc | 0.0397 lb/in³ | ASTM D 792 |
Water Absorption | 0.1 % | 0.1 % | 24 hours @ 73F; ASTM D 570 |
Linear Mold Shrinkage | 0.005 - 0.008 cm/cm | 0.005 - 0.008 in/in | Flow, 0.125 inch; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.005 - 0.007 cm/cm | 0.005 - 0.007 in/in | 0.125 inch; ASTM D 955 |
Melt Flow | 14 g/10 min | 14 g/10 min | 260C/5.0 kgf; ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Break | 44.1 MPa | 6400 psi | Type I, 2.0 in/min; ASTM D 638 |
Tensile Strength @ Yield | 50.3 MPa | 7300 psi | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Break | 150 % | 150 % | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Yield | 8.6 % | 8.6 % | Type I, 2.0 in/min; ASTM D 638 |
Tensile Modulus | 2.14 GPa | 310 ksi | 2.0 in/min; ASTM D 638 |
Flexural Modulus | 2.07 GPa | 300 ksi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Yield Strength | 72.4 MPa | 10500 psi | 0.05 in/min, 2" span; ASTM D 790 |
Izod Impact, Notched, Low Temp | 4.27 J/cm | 8 ft-lb/in | at -22F; ASTM D 256 |
Gardner Impact @ 23°C | 33.9 J | 25 ft-lb | Instrumented Impact Total Energy, -22F; ASTM D 3763 |
Gardner Impact @ 23°C | 40.7 J | 30 ft-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
Izod Impact, Notched | 5.34 J/cm | 10 ft-lb/in | 73F; ASTM D 256 |
Thermal Properties |
|
CTE, linear 68°F | 72 µm/m-°C | 40 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
CTE, linear 68°F, Transverse to Flow | 90 µm/m-°C | 50 µin/in-°F | from -40F to 100F; ASTM E 831 |
Thermal Conductivity | 0.2 W/m-K | 1.39 BTU-in/hr-ft²-°F | ASTM C 177 |
Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | 0.125 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | 0.125 inch, unannealed; ASTM D 648 |
Vicat Softening Point | 112 °C | 233 °F | Rate B; ASTM D 1525 |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|