SABIC Innovative Plastics LEXAN 3412HF Polycarbonate (North America)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
Physical Properties | Metric | English | Comments |
|
Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D 792 |
Linear Mold Shrinkage | 0.002 - 0.004 cm/cm | 0.002 - 0.004 in/in | Flow, 0.125 inch; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm | 0.0045 - 0.0065 in/in | 0.125 inch; ASTM D 955 |
Melt Flow | 8.5 g/10 min | 8.5 g/10 min | 300C/1.2 kgf (O); ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Break | 107 MPa | 15500 psi | Type I, 0.2 in/min; ASTM D 638 |
Tensile Strength @ Yield | 100 MPa | 14500 psi | Type I, 0.2 in/min; ASTM D 638 |
Elongation at Break | 4 % | 4 % | Type I, 0.2 in/min; ASTM D 638 |
Tensile Modulus | 3.45 GPa | 500 ksi | 0.2 in/min; ASTM D 638 |
Flexural Modulus | 5.52 GPa | 800 ksi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Strength | 165 MPa | 24000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Yield Strength | 157 MPa | 22700 psi | 0.05 in/min, 2" span; ASTM D 790 |
Izod Impact, Unnotched | 5.34 J/cm | 10 ft-lb/in | 73F; ASTM D 4812 |
Gardner Impact @ 23°C | 3.39 J | 2.5 ft-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
Izod Impact, Notched | 1.07 J/cm | 2 ft-lb/in | 73F; ASTM D 256 |
Thermal Properties |
|
Deflection Temperature at 0.46 MPa (66 psi) | 142 °C | 287 °F | 0.125 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 138 °C | 280 °F | 0.125 inch, unannealed; ASTM D 648 |
UL RTI, Electrical | 80 °C | 176 °F | UL 746B |
UL RTI, Mechanical with Impact | 80 °C | 176 °F | UL 746B |
UL RTI, Mechanical without Impact | 80 °C | 176 °F | UL 746B |
Flammability, UL94 | V-1 | V-1 | 0.059 in. |
Flammability, UL94 | V-0 | V-0 | 0.118 in. |
Descriptive Properties | |
UL File Number, USA | E121562 | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|