SABIC Innovative Plastics ULTEM AR9300 Polyetherimide (North America)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
Physical Properties | Metric | English | Comments |
|
Density | 1.49 g/cc | 0.0538 lb/in³ | ASTM D 792 |
Linear Mold Shrinkage | 0.002 - 0.004 cm/cm | 0.002 - 0.004 in/in | Flow, 0.125 inch; ASTM D 955 |
Melt Flow | 4.2 g/10 min | 4.2 g/10 min | 337C/6.6 kgf; ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Break | 155 MPa | 22500 psi | Type I, 0.2 in/min; ASTM D 638 |
Elongation at Break | 3 % | 3 % | Type I, 0.2 in/min; ASTM D 638 |
Tensile Modulus | 8.96 GPa | 1300 ksi | 0.2 in/min; ASTM D 638 |
Flexural Modulus | 9.65 GPa | 1400 ksi | 0.10 in/min, 4" span; ASTM D 790 |
Flexural Yield Strength | 241 MPa | 35000 psi | 0.10 in/min, 4" span; ASTM D 790 |
Izod Impact, Notched | 5.34 J/cm | 10 ft-lb/in | Reverse Notched, 73F; ASTM D 256 |
Izod Impact, Notched | 1.17 J/cm | 2.2 ft-lb/in | 73F; ASTM D 256 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 212 °C | 414 °F | 0.250 inch, unannealed; ASTM D 648 |
Flammability Test | 0 | 0 | Vertical Burn, drip time; seconds; FAR 25.853 |
Flammability Test | 0 | 0 | Vertical Burn, extinguish time; seconds; FAR 25.853 |
Flammability Test | 3.5 | 3.5 | Vertical Burn, length; inches; FAR 25.853 |
Flammability Test | 40 | 40 | OSU Peak Heat Release Rate (horizontal); KW/m2; FAR 25.853 |
Flammability Test | 5 | 5 | OSU 2 minute heat, release rate; KW-Min/m2; FAR 25.853 |
NBS Smoke Density | 0 | 0 | Flaming, Ds 1.5 min; ASTM E 662 |
NBS Smoke Density | 5 | 5 | Flaming, Dmax; ASTM E 662 |
NBS Smoke Density | 5 | 5 | Flaming, Ds 4 min; ASTM E 662 |
Descriptive Properties | |
FAR 25.853 | NATURAL | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|