SABIC Innovative Plastics ULTEM HTX1010F Polyetherimide (North America)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
Physical Properties | Metric | English | Comments |
|
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D 792 |
Melt Flow | 15.5 g/10 min | 15.5 g/10 min | 337C/6.6 kgf; ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Break | 82.7 MPa | 12000 psi | Type I, 0.2 in/min; ASTM D 638 |
Tensile Strength @ Yield | 93.1 MPa | 13500 psi | Type I, 0.2 in/min; ASTM D 638 |
Elongation at Break | 40 % | 40 % | Type I, 0.2 in/min; ASTM D 638 |
Tensile Modulus | 3.1 GPa | 450 ksi | 0.2 in/min; ASTM D 638 |
Flexural Modulus | 3.03 GPa | 440 ksi | 0.10 in/min, 4" span; ASTM D 790 |
Flexural Yield Strength | 138 MPa | 20000 psi | 0.10 in/min, 4" span; ASTM D 790 |
Izod Impact, Unnotched | 20.8 J/cm | 39 ft-lb/in | 73F; ASTM D 4812 |
Izod Impact, Notched | 1.6 J/cm | 3 ft-lb/in | 73F; ASTM D 256 |
Izod Impact, Notched | 17.6 J/cm | 33 ft-lb/in | Reverse Notched, 73F; ASTM D 256 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 196 °C | 385 °F | 0.250 inch, unannealed; ASTM D 648 |
Oxygen Index | 39.7 % | 39.7 % | ASTM D 2863 |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|