SABIC Innovative Plastics ULTEM 2100N Polyetherimide (North America)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
| Physical Properties | Metric | English | Comments |
|
| Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D 792 |
| Water Absorption | 0.21 % | 0.21 % | 24 hours @ 73F; ASTM D 570 |
| Water Absorption at Saturation | 1.2 % | 1.2 % | Equilibrium, 73F; ASTM D 570 |
| Linear Mold Shrinkage | 0.005 - 0.006 cm/cm | 0.005 - 0.006 in/in | Flow, 0.125 inch; ASTM D 955 |
| Melt Flow | 7 g/10 min | 7 g/10 min | 337C/6.6 kgf; ASTM D 1238 |
Mechanical Properties |
|
| Hardness, Rockwell M | 114 | 114 | ASTM D 785 |
| Tensile Strength @ Break | 116 MPa | 16800 psi | Type I, 0.2 in/min; ASTM D 638 |
| Tensile Strength @ Yield | 114 MPa | 16600 psi | Type I, 0.2 in/min; ASTM D 638 |
| Elongation at Break | 6 % | 6 % | Type I, 0.2 in/min; ASTM D 638 |
| Tensile Modulus | 4.69 GPa | 680 ksi | 0.2 in/min; ASTM D 638 |
| Flexural Modulus | 5.17 GPa | 750 ksi | 0.10 in/min, 4" span; ASTM D 790 |
| Flexural Strength | 200 MPa | 29000 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Izod Impact, Unnotched | 4.81 J/cm | 9 ft-lb/in | 73F; ASTM D 4812 |
| Izod Impact, Notched | 0.534 J/cm | 1 ft-lb/in | 73F; ASTM D 256 |
| Izod Impact, Notched | 4.59 J/cm | 8.6 ft-lb/in | Reverse Notched, 73F; ASTM D 256 |
Electrical Properties |
|
| Volume Resistivity | 1e+017 ohm-cm | 1e+017 ohm-cm | ASTM D 257 |
| Dielectric Constant | 3.5 | 3.5 | 1 kHz; ASTM D 150 |
| Dielectric Strength | 27.6 kV/mm | 700 V/mil | in oil, 62 mils; ASTM D 149 |
| Dissipation Factor | 0.0014 | 0.0014 | 1 kHz; ASTM D 150 |
| Dissipation Factor | 0.0046 | 0.0046 | 2450 MHz; ASTM D 150 |
Thermal Properties |
|
| CTE, linear, 212°F (100°C) | 32.4 µm/m-°C | 18 µin/in-°F | Flow, 0F to 300F; ASTM E 831 |
| Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | 0.250 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 209 °C | 408 °F | 0.250 inch, unannealed; ASTM D 648 |
| Vicat Softening Point | 223 °C | 434 °F | Rate B; ASTM D 1525 |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to