SABIC Innovative Plastics ULTEM 2210 Polyetherimide (North America)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
| Physical Properties | Metric | English | Comments |
|
| Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D 792 |
| Melt Flow | 8.4 g/10 min | 8.4 g/10 min | 337C/6.6 kgf; ASTM D 1238 |
Mechanical Properties |
|
| Hardness, Rockwell M | 114 | 114 | ASTM D 785 |
| Tensile Strength @ Break | 140 MPa | 20300 psi | Type I, 0.2 in/min; ASTM D 638 |
| Elongation at Break | 4 % | 4 % | Type I, 0.2 in/min; ASTM D 638 |
| Tensile Modulus | 6.89 GPa | 1000 ksi | 0.2 in/min; ASTM D 638 |
| Flexural Modulus | 6.89 GPa | 1000 ksi | 0.10 in/min, 4" span; ASTM D 790 |
| Flexural Strength | 228 MPa | 33000 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Izod Impact, Unnotched | 4.75 J/cm | 8.9 ft-lb/in | 73F; ASTM D 4812 |
| Izod Impact, Notched | 0.641 J/cm | 1.2 ft-lb/in | 73F; ASTM D 256 |
| Izod Impact, Notched | 4.54 J/cm | 8.5 ft-lb/in | Reverse Notched, 73F; ASTM D 256 |
Electrical Properties |
|
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten (+/- 0.125 inch); PLC Code 6; ASTM D 495 |
| Comparative Tracking Index | 100 - 175 V | 100 - 175 V | (+/- 0.125 inch); PLC Code 4; UL 746A |
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | (+/- 0.125 inch); PLC Code 1; UL 746A |
| High Amp Arc Ignition, HAI | Max 15 arcs | Max 15 arcs | Surface (+/- 0.125 inch); PLC Code 4; UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80 mm/min | 1 - 3.15 in/min | (+/- 0.125 inch); PLC Code 2; UL 746A |
Thermal Properties |
|
| Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | 0.250 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 211 °C | 412 °F | 0.250 inch, unannealed; ASTM D 648 |
| Vicat Softening Point | 226 °C | 438 °F | Rate B; ASTM D 1525 |
| UL RTI, Electrical | 170 °C | 338 °F | UL 746B |
| UL RTI, Mechanical with Impact | 170 °C | 338 °F | UL 746B |
| UL RTI, Mechanical without Impact | 170 °C | 338 °F | UL 746B |
| Flammability, UL94 | V-0 | V-0 | 0.016 in. |
| Flammability, UL94 | 7 | 7 | 0.075 in. |
| NBS Smoke Density | 1.3 | 1.3 | Flaming, Ds 4 min; ASTM E 662 |
| NBS Smoke Density | 27 | 27 | Flaming, Dmax 20 min; ASTM E 662 |
| Oxygen Index | 50 % | 50 % | ASTM D 2863 |
Descriptive Properties | |
| UL File Number, USA | E121562 | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|